FIPC Formosa TARFLON™ IV1900R

FIPC Tarflon IV1900R

TARFLON™ IV1900R PC Resin Weathering Grade UV-stabilized

Tarflon IV1900R is a UV-stabilized polycarbonate resin offering exceptional clarity, durability, and mold release properties. Ideal for automotive and outdoor applications, it combines high impact resistance (70 kJ/m²), UV protection (cut-off <380 nm), and compliance with AMECA and UL f1 standards, ensuring reliability in harsh environments.

  • Manufacturer: Formosa Idemitsu Petrochemical Corporation (FIPC)
  • Character: UV-stabilized PC with UV cut-off under 380 nm, iced-clear color, and good mold release property. IV-R grade is listed in AMECA
  • Application: for car headlamp, lighting equipment and various outdoor applications
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Melt Flow Rate (MFR): 19 g/10min
  • Tensile Strength: 65 MPa
  • Impact Resistance: 70 kJ/m²
  • Heat Resistance: HDT 125°C (1.8 MPa)
  • UV Stability: AMECA-listed, UL f1-rated
  • Molding Parameters: Pre-dry at 120°C (5–8hrs); mold at 80–120°C.

Superior UV Resistance & Clarity

Tarflon IV1900R blocks harmful UV rays below 380 nm while maintaining 85–90% light transmittance. This ensures long-term color stability and prevents yellowing, perfect for automotive headlamps and outdoor lighting exposed to sunlight.

High Impact Strength

With a Charpy impact strength of 70 kJ/m², this Tarflon polycarbonate resists cracking under stress, reducing failure risks in components like vehicle housings or rugged outdoor equipment.

Efficient Mold Release

The resin’s excellent flow (MFR 19 g/10min) and low mold shrinkage (0.5–0.7%) streamline production, cutting cycle times and costs for high-volume parts like lenses or enclosures.

FIPC Tarflon PC resin

Application

  • Automotive Lighting: AMECA-certified for headlamps, fog lights, and signal covers.
  • Outdoor Equipment: UV-resistant enclosures for LED streetlights or solar panels.
  • Industrial Components: High-impact housings for machinery and electrical systems.
  • Consumer Electronics: Durable, clear covers for displays or touchscreens.
Tarflon IV1900R PC resin application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top