FIPC Formosa TARFLON™ VT2500

FIPC Tarflon VT2500

TARFLON™ VT2500 PC Resin Weathering Grade UV-stabilized

Tarflon VT2500 is a UV-stabilized polycarbonate resin engineered for demanding applications requiring clarity, durability, and weatherability. With a UV cutoff below 400 nm, it offers long-term protection against yellowing while maintaining an iced-clear appearance. Ideal for transparent components exposed to harsh environments.

  • Manufacturer: Formosa Idemitsu Petrochemical Corporation (FIPC)
  • Character: UV-stabilized PC with UV cut-off under 400 nm, iced-clear color and good mold release property.
  • Application: for safety glasses, sun glasses and daylight roof
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Mechanical Strength: Tensile stress at yield = 65 MPa | Flexural modulus = 2.2 GPa
  • Impact Performance: Charpy notched impact = 80 kJ/m²
  • Thermal Stability: Heat deflection temperature = 125°C (1.8 MPa)
  • Optical Clarity: 85–90% luminous transmittance with UV protection
  • Molding Parameters: Pre-dry at 120°C for 5–8 hours; Cylinder temp: 260–300°C | Mold temp: 80–120°C

Advanced UV Protection

Tarflon VT2500 blocks harmful UV rays below 400 nm, preventing yellowing and degradation. This ensures products like safety glasses or daylight roofs retain clarity and structural integrity even after prolonged sun exposure.

Exceptional Impact Resistance

With a Charpy impact strength of 80 kJ/m², this Tarflon polycarbonate resists cracks and fractures under stress. Ideal for protective gear or automotive parts requiring lightweight yet rugged performance.

Streamlined Manufacturing

Excellent mold release properties minimize sticking, reducing cycle times and defects. Coupled with easy processing (MFR: 7 g/10min), it enables faster, cost-effective production of precision components.

FIPC Tarflon PC resin

Application

  • Safety Glasses: Combines UV resistance with impact protection for worker safety.
  • Sunglasses: Maintains clarity and blocks harmful rays for outdoor eyewear.
  • Daylight Roofs: Offers durability, transparency, and long-term weatherability for automotive or architectural use.
Tarflon VT2500 PC resin application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top