LEXAN™ PC Resin 121M

LEXAN™ PC Resin Sabic Tianjin

SABIC PC Lexan 121M General Purpose Grade

LEXAN 121M is a versatile 18 MFR polycarbonate resin. It features improved internal mold release for higher productivity and carries a UL94 HB flammability rating for general applications.

  • Character: 18 MFR, UL94 HB rated
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 63 MPa
  • Flexural Modulus: 2350 MPa
  • Notched Izod Impact (23°C): 820 J/m
  • Heat Deflection Temp (1.82 MPa): 132°C
  • Vicat Softening Temperature: 143°C
  • Melt Flow Rate (300°C/1.2kg): 17.5 g/10 min
  • Specific Gravity: 1.20
  • Mold Shrinkage: 0.5 – 0.8 %
  • Light Transmission (2.54mm): 88%
  • UL94 Rating: HB

Application

  • Consumer Electronics Housings
  • Automotive Interior Components
  • Lighting Fixtures and Diffusers
  • Appliance Housings and Parts
  • General Industrial Components

Features & Benefits

Enhanced Mold Release Efficiency

This LEXAN™ 121M resin contains an internal mold release agent, which reduces cycle times and increases output by allowing for easier part ejection, saving you time and cost.

Superior Impact Resistance & Strength

It offers excellent toughness and high tensile strength, ensuring your products can withstand everyday impacts and stresses without cracking or failing, enhancing durability.

High Heat Resistance & Clarity

With a Heat Deflection Temperature of 132°C and 88% light transmission, it is ideal for applications requiring both thermal stability and optical clarity for a premium look.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top