Sabic LEXAN™ PC Resin 121SRM

sabic pc resin 25kg package

SABIC PC Lexan 121SRM General Purpose Grade

LEXAN 121SRM is an easy-flow, impact-modified, and super-release grade polycarbonate resin, designed for high-volume, complex injection molding with exceptional demolding.

Associated Documents

TDS Asia

Typical property data

Physical Properties
  • Specific Gravity: 1.2 (ASTM D792)
  • Water Absorption (23°C/24 hrs): 0.15% (ASTM D570)
  • Mold Shrinkage, flow, 3.2 mm: 0.5 – 0.7% (SABIC Method)
  • Melt Flow Rate, 300°C/1.2 kgf: 18 g/10 min (ASTM D1238)
Mechanical Properties
  • Tensile Stress, Yield, Type I, 50 mm/min: 65 MPa (ASTM D638)
  • Tensile Strain, Break, Type I, 50 mm/min: 143% (ASTM D638)
  • Flexural Stress, Yield, 1.3 mm/min, 50 mm span: 97 MPa (ASTM D790)
  • Flexural Modulus, 1.3 mm/min, 50 mm span: 2300 MPa (ASTM D790)
Impact Properties
  • Izod Impact, Notched, 23°C: 801 J/m (ASTM D256)
Thermal Properties
  • Heat Deflection Temperature (HDT), 1.82 MPa, 3.2 mm, Unannealed: 123°C (ASTM D648)
  • Heat Deflection Temperature (HDT), 1.82 MPa, 6.4 mm, Unannealed: 133°C (ASTM D648)
Injection Molding
  • Drying Temperature: 120°C
  • Drying Time: 3 – 4 hours
  • Cumulative Drying Time: 48 hours
  • Melt Temperature: 280 – 305°C
  • Mold Temperature: 70 – 95°C

Features & Benefits

Superior Mold Release

This LEXAN 121SRM resin significantly reduces ejection forces, preventing part sticking and deformation for faster cycle times and lower scrap rates.

Exceptional Impact Resistance

With a high notched Izod impact strength, LEXAN™ 121SRM resin produces durable components that can withstand sudden impacts and rough handling in demanding environments.

Excellent Flow & Processability

The easy-flow nature of this PC resin ensures complete filling of intricate and thin-walled molds, resulting in fewer short shots and improved surface finish.

sabic pc resin 25kg package

Use & Applications

  • Thin-walled and complex consumer electronics housings
  • Durable components for power tools and appliances
  • Automotive interior parts and connectors
  • High-volume production parts requiring fast cycle times
sabic pc resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.