LEXAN™ PC Resin 124R

LEXAN™ PC Resin Sabic Tianjin

SABIC PC Lexan 124R General Purpose Grade

LEXAN 124R resin is an 18 MFR polycarbonate with mold release. It is UL94 HB rated and offers food contact compliance in most regions, making it a versatile and reliable engineering plastic.

  • Character: 18 MFR, 21 MVR, Mold release, UL94 HB rated.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 62 MPa
  • Flexural Modulus: 2340 MPa
  • Notched Izod Impact (23°C): 694 J/m
  • Rockwell Hardness (M Scale): 70
  • Heat Deflection Temp (1.82 MPa): 129 °C
  • Vicat Softening Temperature: 154 °C
  • Relative Temperature Index (Elec/Mech): 130 °C
  • Melt Flow Rate (300°C/1.2kg): 17.5 g/10 min
  • Mold Shrinkage: 0.5 – 0.7 %
  • Specific Gravity: 1.20
  • Light Transmission (2.54mm): 88%
  • UL94 Flame Rating: HB
  • Melt Temperature: 280 – 305 °C
  • Mold Temperature: 70 – 95 °C
  • Drying: 3-4 hours at 120°C

Application

  • Food Storage Containers and Lids
  • Small Kitchen Appliances (Housings & Components)
  • Consumer Electronics Housings
  • Thin-Wall Packaging
  • Light Diffusers and Covers
  • Office Equipment Housings
  • Medical Device Housings (non-critical)
  • Automotive Interior Trim Components

Features & Benefits

Built-In Mold Release Agent

This feature significantly reduces cycle times and improves part ejection, leading to higher productivity and lower per-part costs for high-volume injection molding.

Excellent Impact Strength & Toughness

Its high notched Izod impact resistance ensures your products can withstand rough handling and accidental drops, enhancing durability and reducing failure rates.

High Clarity & Food Contact Potential

With 88% light transmission and compliance with food contact regulations in most areas, it is an ideal, safe choice for transparent food containers, lids, and kitchenware.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity