Polylac® PA-737 A03 Standard Color Medium Impact
POLYLAC PA-737 A03 is a high-flow, medium-impact White ABS resin engineered for demanding applications. Combining exceptional moldability with durability, this Chimei POLYLAC® ABS grade simplifies production of large or thin-walled parts while maintaining structural integrity. Ideal for appliances and electronics.
- Application: Home appliance/Large area or thin-wall molded products
- Character: High flow/Medium Impact
Key technical data (ISO)
- Melt Flow Index: 30 ml/10 min (220°C/10kg)
- Izod Impact Strength: 19 KJ/m² (23°C, notched)
- Vicat Softening Temp: 104°C (1kg load)
- Flammability Rating: UL94 HB (1.5mm)
- Mold Shrinkage: 0.4–0.7%

Applications
POLYLAC® PA-737 A03 solves challenges in industries requiring precision, speed, and reliability:
- Home Appliances: Refrigerator liners, washing machine panels, and air conditioner vents (resists warping and cracks).
- Thin-Wall Electronics: Printer housings, laptop bases (high flow prevents sink marks).
- Large-Area Parts: Vacuum cleaner bodies, automotive trim (uniform finish with minimal shrinkage).

Polylac® PA-737 A03 Datasheet
| White ABS POLYLAC® PA-737_A03 Product Description: High flow, Medium impact | ||||
| Properties | ISO Test Method | Test Condition | Unit | PA-737_A03 |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 30 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.04 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 38 |
| 50 mm/min, break | MPa | 31 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 20 |
| Flexural Strength | 178 | 2 mm/min | MPa | 59 |
| Flexural Modulus | 2 mm/min | GPa | 1.9 | |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 19 |
| -30℃, Notched | KJ/m2 | 9 | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 19 |
| -30℃, Notched | KJ/m2 | 9 | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 104 |
| 50℃/hr;5KG | ℃ | 97 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 81 |
| 1.8MPa, annealed | ℃ | 96 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 8.2 x 10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB |
| Mold Shrinkage | 294-4 | – | % | 0.4~0.7 |
| Symbol | 1043 | – | – | >ABS< |
| March 12, 2025 Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test | ||||
Polylac® PA-737 A03 UL Product iQ
| POLYLAC® PA-737 | UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets |
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 4 | |
| 3.0 mm | PLC 4 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| Comparative Tracking Index (CTI) | PLC 1 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 0 | |
| High Voltage, Low Current Arc Resistance | PLC 7 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
Related Polylac® ABS Plastics
Chimei Polylac® PA-763AH ABS
Chimei Polylac® PA-763H ABS
Chimei Polylac® PA-764B
Chimei Polylac® PA-764G
Chimei Polylac® PA-797 ABS
Chimei Polylac® PA-757G J08 ABS
Chimei Polylac® PA-757 J01 ABS
Chimei Polylac® PA-757 A01 ABS
Chimei Polylac® PA-756S ABS
Chimei Polylac® PA-756H ABS
Chimei Polylac® PA-747S A01 ABS
Chimei Polylac® PA-747S ABS
Chimei Polylac® PA-747R ABS
Chimei Polylac® PA-747H ABS
Chimei Polylac® PA-747F ABS
Chimei Polylac® PA-746M ABS
Chimei Polylac® PA-746H ABS
Chimei Polylac® PA-737 A03 ABS