FIPC Formosa TARFLON™ IV2200R

FIPC Tarflon IV2200R

TARFLON™ IV2200R PC Resin Weathering Grade UV-stabilized

Tarflon IV2200R is a UV-stabilized polycarbonate resin engineered for demanding outdoor and automotive applications. With a UV cut-off under 380 nm, iced-clear transparency, and exceptional impact resistance (80 kJ/m²), it delivers long-term durability and optical clarity. Ideal for headlamps, lighting, and components requiring structural integrity, it combines easy mold release with UL f1 certification for reliability in harsh environments.

  • Manufacturer: Formosa Idemitsu Petrochemical Corporation (FIPC)
  • Character: UV-stabilized PC with UV cut-off under 380 nm, iced-clear color, and good mold release property. IV-R grade is listed in AMECA.
  • Application: for car headlamp, lighting equipment and various outdoor applications
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Tensile Strength: 65 MPa
  • Flexural Modulus: 2.3 GPa
  • Impact Resistance: 80 kJ/m²
  • Heat Deflection Temp: 125°C
  • UL f1 Rated (UV/weather resistance) | AMECA Listed
  • Optical Clarity: 85–90% luminous transmittance

UV Resistance That Lasts

Tarflon IV2200R’s UV stabilization blocks harmful wavelengths below 380 nm, preventing yellowing and brittleness. This ensures outdoor lighting housings or automotive lenses stay crystal-clear for years, reducing replacement costs.

Built to Withstand Impact

With Charpy impact strength of 80 kJ/m², this Tarflon polycarbonate resists cracking under stress. Perfect for rugged applications like machinery guards or vehicle components exposed to vibrations and shocks.

Effortless High-Performance Molding

Excellent mold release properties and low shrinkage (0.5–0.7%) streamline production. Mold complex parts like intricate headlamp bezels faster, minimizing downtime and achieving consistent quality.

FIPC Tarflon PC resin

Application

  • Automotive: AMECA-listed for headlamp lenses, bezels, and housings.
  • Lighting: UV-resistant covers for LED streetlights or stadium fixtures.
  • Outdoor Equipment: Durable panels for solar enclosures or signage.
  • Industrial: Transparent machine guards requiring impact resistance and clarity.
Tarflon IV2200R PC resin application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top