FIPC Formosa TARFLON™ MD1500

FIPC Tarflon MD1500

TARFLON™ MD1500 PC Resin Optical Grade Optical Disc Molding

Tarflon MD1500 is a high-flow, low-contamination tarflon polycarbonate resin engineered for precision optical media like CDs, DVDs, and Blu-ray discs. Combining superior transparency (85–90% light transmittance) with exceptional mechanical strength (65 MPa tensile stress) and ultra-low viscosity, it enables stable, high-speed molding for flawless production.

  • Manufacturer: Formosa Idemitsu Petrochemical Corporation (FIPC)
  • Character: Optical PC with high-flow and low-level contamination
  • Application:  for optical media such as CD, DVD and BD. 
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Rate: 65 g/10min
  • Mechanical Strength: 65 MPa tensile stress, 15 kJ/m² impact resistance
  • Thermal Stability: 125°C heat deflection
  • Optical Clarity: 85–90% light transmittance
  • Processing: Pre-dry at 120°C for 5–8 hours; mold at 80–120°C

High-Flow Optical Precision

Tarflon MD1500’s ultra-low viscosity ensures seamless flow into intricate molds, reducing bubbles and defects in optical discs. This guarantees crisp data replication and minimal waste.

Stable High-Temperature Molding

With a heat deflection temperature of 125°C, this tarflon polycarbonate maintains structural integrity during high-speed processing, cutting cycle times without compromising disc durability.

Crystal-Clear Transparency

It achieve 85–90% luminous transmittance for sharper readability in media applications. Its low contamination profile ensures discs stay pristine, even under prolonged UV exposure.

FIPC Tarflon PC resin

Application

  • CD/DVD Replication Layers
  • Blu-ray Disc Coatings
  • Industrial-Grade Optical Media
  • Protective Film Layers
Tarflon MD1500 PC resin application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top