FIPC Formosa TARFLON™ LC1500

FIPC Tarflon LC1500

TARFLON™ LC1500 Light Guide Grade PC Panel Daytime Running Light

Tarflon LC1500 is a high-flow, low-contamination polycarbonate resin engineered for precision light guide panels and automotive daytime running lights. With exceptional light transmission (90%) and robust mechanical strength, it ensures durability and optical clarity in demanding applications.

  • Manufacturer: Formosa Idemitsu Petrochemical Corporation (FIPC)
  • Characte: high-flow, High Optical Clarity
  • Application: Light-conduct PC, Light Guide Plate, LGP, LCD
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Melt Flow Rate: 65 g/10min
  • Tensile Strength: 65 MPa
  • Impact Resistance: 15 kJ/m²
  • Heat Resistance: 127°C
  • Light Transmission: 90%
  • Molding Temp Range: 240–260°C

Superior Flow for Complex Molds

Tarflon LC1500’s high melt flow rate (65 g/10min) enables seamless filling of intricate molds, reducing cycle times and minimizing defects in thin-walled or detailed designs like automotive LED housings.

Optical Clarity

Low contamination levels and 90% luminous transmittance ensure consistent light diffusion, ideal for backlit displays or automotive lighting where brightness uniformity is critical.

Toughness Meets Precision

Balancing impact resistance (15 kJ/m²) and rigidity (2.3 GPa flexural modulus), Tarflon polycarbonate withstands mechanical stress while maintaining dimensional stability in harsh environments.

FIPC Tarflon PC resin

Application

  • Automotive Lighting: Daytime running lights (DRLs) requiring high brightness and heat resistance.
  • Consumer Electronics: Light guide panels for LCD displays, ensuring even backlighting.
  • Industrial Sensors: Housings for optical sensors needing contamination-free clarity.
Tarflon LC1500 PC resin application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top