FCFC Formosa TAIRILITE® AC2916
TAIRILAC® AC2916 PC Resin High Transparency Grade Tairilite AC2916 is a premium-grade polycarbonate resin engineered for high transparency and exceptional flow properties. Ideal for precision injection molding, TAIRILITE PC RESIN delivers outstanding optical clarity (>90% transmission) and process efficiency, making it perfect for demanding applications like automotive lighting and optical components. Key technical data (ISO)
FCFC Formosa TAIRILITE® AC2916 Read More »