Chimei Polylac® PA-763AH ABS

Chimei POLYLAC PA-763AH ABS plastic

Polylac® PA-763AH Flame Retardant Grade ABS Plastic


CHIMEI POLYLAC® PA-763AH is a high-flow, flame-retardant ABS resin engineered for demanding applications. With certifications like 2.0mm V-0, 5VB, and 5VA, it combines heat resistance (102°C Vicat), light stability, and superior moldability—ideal for thin-walled parts requiring safety, durability, and precision.

  • Character: High-flowability, Light-resistance, heat-resistance, 2.0mm V-0, 2.0mm 5VB, 2.5mm 5VA (Non-TBBA series)
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 45 ml/10 min, ISO 1133 (220°C/10KG)
  • Tensile Strength: 40 MPa (Yield), ISO 527
  • Izod Impact (23°C): 16 KJ/m², ISO 180
  • Heat Distortion Temp.: 76°C (1.8MPa, unannealed), ISO 75/A
  • Flammability: 2.0mm V-0, 5VB; 2.5mm 5VA, UL 94, IEC 60695
  • Mold Shrinkage: 0.3–0.6%, ISO 294-4

Superior Flame Retardancy

PA-763AH meets UL 94 V-0 (2.0mm), 5VB, and 5VA standards, ensuring compliance with global safety regulations. Perfect for electronics and automotive parts where fire resistance is critical.

High Flowability for Efficiency

With a melt flow index of 45 ml/10 min, it fills complex molds quickly, reducing cycle times and energy costs. Ideal for intricate components like printer casings or power outlets.

Heat & Light Resilience

Vicat softening at 102°C and UV resistance ensure long-term stability in harsh environments. Use for outdoor displays, car audio consoles, or appliances exposed to heat and sunlight.

Chimei POLYLAC PA-763AH ABS

Applications

  • Electronics & IT: Modems, power panels, printer casings, projectors.
  • Appliances: Coffee machines, TV frames, DVD players, fax machines.
  • Automotive: Car batteries, audio consoles, light boxes.
  • Industrial: Machine enclosures, cash register shells, multifunctional peripherals.
Chimei POLYLAC PA-763AH application

Polylac® PA-763AH Datasheet

Flame Retardant ABS POLYLAC®  PA-763AH
Product Description: F.R. High flow,High heat,Weather resistant
PropertiesISO Test MethodTest ConditionUnitPA-763AH
Melt Flow Index1133 220℃×10KGml/10 min45 
Mass Density1183 23 ℃g/cm31.18 
Tensile Strength527 50 mm/min, yieldMPa40 
50 mm/min, breakMPa29 
Tensile Elongation527 50 mm/min%13 
Flexural Strength178 2 mm/minMPa60 
Flexural Modulus2 mm/minGPa2.0 
Izod Impact Strength180/1A23℃, NotchedKJ/m216 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m216 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG102 
50℃/hr;5KG91 
Heat Distortion Temp.75/A1.8MPa, unannealed76 
1.8MPa, annealed92 
Coefficient of Linear Thermal Expansion11359 8.45 x 10-5
FlammabilityUL-942.0mm V-0
2.0mm 5VB
2.5mm 5VA
Mold Shrinkage294-4%0.3~0.6
Symbol1043 >ABS-FR(17)<
March  12, 2025
Notes:These are typical properties only and are not to be construed as specifications. Users
should confirm results by their own test

Polylac® PA-763AH UL Product iQ

POLYLAC® PA-763AH | UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
2.0 mm, Color: ALL5VB, V-0
2.5 mm, Color: ALL5VA, V-0
3.0 mm, Color: ALL5VA, V-0
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
2.0 mm, Color: ALLV-0
2.5 mm, Color: ALLV-0
3.0 mm, Color: ALLV-0
FlammabilityIEC 60695-11-20
2.0 mm, Color: ALL5VB
2.5 mm, Color: ALL5VA
3.0 mm, Color: ALL5VA
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
2.0 mmPLC 3
2.5 mmPLC 2
3.0 mmPLC 2
High Amp Arc Ignition (HAI)UL 746A
2.0 mmPLC 2
2.5 mmPLC 2
3.0 mmPLC 2
Comparative Tracking Index (CTI)PLC 2UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 4
High Voltage, Low Current Arc ResistancePLC 5
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
2.0 mm60   °C
2.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical ImpactUL 746B
2.0 mm60   °C
2.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical StrengthUL 746B
2.0 mm60   °C
2.5 mm60   °C
3.0 mm60   °C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top