Chimei Polylac® PA-764B

Chimei POLYLAC PA-764B ABS plastic

Polylac® PA-764B Flame Retardant Grade ABS Plastic


CHIMEI POLYLAC® PA-764B is a flame-retardant ABS resin engineered for durability and safety. With UL 94 certifications (2.5mm V-0, 5VB; 3.0mm 5VA), it excels in heat resistance (HDT up to 93°C) and impact strength, ideal for electrical enclosures, automotive components, and appliances. Weather-resistant and UL-compliant, it balances performance with regulatory compliance.

  • Character Description: Light resistance, heat resistance 2.5mm V-0, 2.5mm 5VB, 3.0mm 5VA
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 26 ml/10 min (220°C/10kg)
  • Flammability: UL 94 V-0 (2.5mm), 5VB (2.5mm), 5VA (3.0mm).
  • Heat Resistance: HDT 83–93°C (1.8MPa); Vicat Softening Temp: 102°C.
  • Impact Strength: 14 KJ/m² (Izod, 23°C)
  • Mold Shrinkage: 0.3–0.6%
  • Certifications: UL 746A/B, IEC 60695 compliant.

Superior Flame Retardancy

POLYLAC PA-764B meets stringent UL 94 V-0, 5VB, and 5VA standards, ensuring fire safety in thin-walled applications like power panels or electronics housings. Reduces fire risks without compromising structural integrity.

Robust Mechanical Durability

With tensile strength up to 37 MPa and impact resistance (14 KJ/m² at 23°C), it withstands drops, vibrations, and daily wear. Perfect for printer casings, car audio consoles, or industrial equipment.

Reliable Heat Resistance

Vicat softening temperature of 102°C and HDT up to 93°C ensure stability in high-heat environments, such as coffee machines or automotive battery housings. Minimizes warping and deformation.

Chimei POLYLAC PA-764B ABS

Applications

  • Electronics: Modems, power outlets, remote controls, DVD players.
  • Industrial Equipment: Machine boxes, cash register shells, projectors.
  • Automotive: Car battery housings, audio consoles.
  • Appliances: Coffee machines, front/rear TV frames, light boxes.
  • Office Tech: Printer casings, fax machines, multifunctional peripherals.
Chimei POLYLAC PA-764B application

Polylac® PA-764B Datasheet

Flame Retardant ABS POLYLAC®  PA-764B
Product Description: F.R. Weather resistant
PropertiesISO Test MethodTest ConditionUnitPA-764B
Melt Flow Index1133 220℃×10KGml/10 min26 
Mass Density1183 23 ℃g/cm31.16 
Tensile Strength527 50 mm/min, yieldMPa37 
50 mm/min, breakMPa29 
Tensile Elongation527 50 mm/min%15 
Flexural Strength178 2 mm/minMPa57 
Flexural Modulus2 mm/minGPa1.8 
Izod Impact Strength180/1A23℃, NotchedKJ/m214 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m214 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG102 
50℃/hr;5KG90 
Heat Distortion Temp.75/A1.8MPa, unannealed83 
1.8MPa, annealed93 
Coefficient of Linear Thermal Expansion11359 8.63 x 10-5
FlammabilityUL-942.5mm V-0
2.5mm 5VB
3.0mm 5VA
Mold Shrinkage294-4%0.3~0.6
Symbol1043 >ABS-FR(17)<
March  12, 2025
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

Polylac® PA-764B UL Product iQ

POLYLAC® PA-764B(+) | UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
(+) – Indicate 0~0.5% acid scavengers.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
2.5 mm, Color: ALL5VB, V-0
3.0 mm, Color: ALL5VA, V-0
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
2.5 mm, Color: ALLV-0
3.0 mm, Color: ALLV-0
FlammabilityIEC 60695-11-20
2.5 mm, Color: ALL5VB
3.0 mm, Color: ALL5VA
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
2.5 mmPLC 4
3.0 mmPLC 3
High Amp Arc Ignition (HAI)UL 746A
2.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 0UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 2
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
2.5 mm75   °C
3.0 mm80   °C
Relative Thermal Index – Mechanical ImpactUL 746B
2.5 mm80   °C
3.0 mm80   °C
Relative Thermal Index – Mechanical StrengthUL 746B
2.5 mm75   °C
3.0 mm80   °C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top