Chimei Polylac® PA-797 ABS

Chimei POLYLAC PA-797 ABS plastic

Polylac® PA-797 Chemical Resistance Grade High Impact


Chimei POLYLAC PA-797 is a high-performance CHIMEI POLYLAC® ABS resin engineered for chemical endurance and high impact resistance. Ideal for demanding applications, this material combines durability with versatility, making it a reliable choice for kitchen appliances, industrial components, and household products that face harsh environments.

  • Character Description: Chemical resistance and high impact resistance
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 9.2 ml/10 min (220°C)
  • Tensile Strength: 43 MPa (Yield)
  • Heat Resistance: 80°C Heat Distortion Temperature (1.8MPa)
  • Flammability: UL94 HB (1.5mm)
  • Mold Shrinkage: 0.4–0.7%

Superior Chemical Resistance

POLYLAC PA-797 excels in environments exposed to oils, detergents, and cleaning agents. Its chemical endurance ABS formulation prevents degradation, ensuring long-lasting performance for dishwasher components or kitchenware.

Unmatched Impact Strength

With 35 KJ/m² Izod Impact Strength (23°C), this Chimei PA-797 resin withstands drops, shocks, and rough handling. Perfect for appliance housings or tool handles that demand toughness.

Reliable Thermal Stability

It maintains structural integrity up to 105°C Vicat Softening Temperature, ideal for parts near heat sources like microwave panels or coffee maker housings.

Chimei POLYLAC PA-797 ABS

Applications

  • Blender and Mixer Housings – Withstands impacts and resists grease/oil splatter.
  • Refrigerator Interior Parts – Endures repeated exposure to cleaning chemicals.
  • Small Appliance Panels – Retains shape under heat (e.g., toasters, air fryers).
  • Dishwasher Components – Resists steam and detergent corrosion.
Chimei POLYLAC PA-797application

Polylac® PA-797 Datasheet

Chemical resistance ABS POLYLAC®  PA-797
Product Description: Chemical Endurance
PropertiesISO Test MethodTest ConditionUnitPA-797
Melt Flow Index1133 220℃×10KGml/10 min9.2 
Mass Density1183 23 ℃g/cm31.05 
Tensile Strength527 50 mm/min, yieldMPa43 
50 mm/min, breakMPa33 
Tensile Elongation527 50 mm/min%30 
Flexural Strength178 2 mm/minMPa51 
Flexural Modulus2 mm/minGPa1.1 
Izod Impact Strength180/1A23℃, NotchedKJ/m235 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m235.5 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG105 
50℃/hr;5KG95 
Heat Distortion Temp.75/A1.8MPa, unannealed80 
1.8MPa, annealed99 
Coefficient of Linear Thermal Expansion11359 8.8 x 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.7
Symbol1043 >ABS<
March  12, 2025
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

Polylac® PA-797 UL Product iQ

POLYLAC® PA-797 | UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 5
3.0 mmPLC 4
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 0UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 0
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity