Chimei WONDERLITE® PC-110

CHIMEI-WONDERLITE-PC-110

WONDERLITE® PC-110 General Purpose grade Resin Medium viscosity Plastic

Chimei WONDERLITE® PC-110 is a high-performance polycarbonate resin that delivers exceptional clarity and durability. This versatile PC resin is perfect for injection molding applications where transparency meets strength. From automotive lighting to food containers and fashion accessories, PC-110 offers reliable performance and consistent quality.

  • Manufacturer: CHIMEI
  • Application: General injection molding for vehicle indicator light casings, chocolate containers, high heel shoes
  • Character: Weather and UV resistant formulation, medium viscosity for easy processing
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.

Chimei WONDERLITE® PC-110 Application

Superior Clarity Meets Impact Resistance

PC-110 polycarbonate resin delivers exceptional transparency while maintaining outstanding impact strength, making it perfect for demanding visual and structural applications.

Easy Processing for Consistent Results

With medium viscosity and excellent flow properties, Chimei PC-110 ensures smooth injection molding performance and reliable production quality every time.

Versatile Applications Across Many Industries

From automotive indicator lights to food-grade containers and fashion accessories, this polycarbonate resin adapts to diverse manufacturing needs with consistent results.

PC Resin Chimei PC-110

WONDERLITE® PC-110 Datasheet

General PC WONDERLITE® PC-110
Product Description: Medium viscosity
PropertiesISO Test MethodTest ConditionUnitPC-110
Melt Flow Index1133300℃  × 1.2KGml/10 min10
Mass Density118323  ℃g/cm31.2
Tensile Strength52750 mm/min, yieldMPa65
50 mm/min, breakMPa75
Tensile Elongation52750 mm/min%120
Flexural Strength1782 mm/minMPa90
Flexural Modulus1782 mm/minGPa2.4
Izod Impact Strength180/1A23℃, Notched,1/8″KJ/m275
-30℃, Notched,1/8″KJ/m2
Charpy Impact Strength17923℃, NotchedKJ/m275
-30℃, NotchedKJ/m2
Vicat Softening Temp.30650℃/hr;1KG150
50℃/hr;5KG145
Heat Distortion Temp.75/A1.8MPa, unannealed128
1.8MPa, annealed143
Coefficient of Linear Thermal Expansion113596.0~8.0×10-5
FlammabilityUL-942.5mm V-2
Mold Shrinkage294-4%0.5~0.7
Symbol1043>PC<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

WONDERLITE® PC-110 UL Product iQ

WONDERLITE® PC-110 UL Product iQ
File Number: E56070Yellow Card™Polycarbonate (PC) “WONDERLITE”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLV-2
2.5 to 2.8 mm, Color: ALLV-2
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLV-2
2.5 to 2.8 mm, Color: ALLV-2
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 2
2.5 to 2.8 mmPLC 2
3.0 mmPLC 2
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 4
2.5 to 2.8 mmPLC 3
3.0 mmPLC 3
Comparative Tracking Index (CTI)PLC 2UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 2
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm125   °C
2.5 to 2.8 mm125   °C
3.0 mm125   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm105   °C
2.5 to 2.8 mm105   °C
3.0 mm105   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm125   °C
2.5 to 2.8 mm125   °C
3.0 mm125   °C
Report Date: 2001-09-25

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top