Chimei WONDERLITE® PC-122u

Chimei-WONDERLITE-PC-122U

WONDERLITE® PC-122U Weathering Grade UV Stabilized

Wonderlite PC-122U is a high-flow polycarbonate resin made by CHIMEI. It’s great for making thin, see-through items like pen tubes, toys, and water bottles. The resin is tough, bends without breaking, and can handle heat well. It’s also UV-stable, making it good for outdoor use. Wonderlite PC-122U is easy to mold into complex shapes, perfect for creating clear, durable products.

  • Application: Outdoor applications, traffic signs
  • Character: UV Stabilized
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides. All documents are sourced directly from manufacturers.

Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
Chimei WONDERLITE® PC-122U Application

Superior Flow for Complex Molding

Wonderlite PC-122U’s high flow properties (22 ml/10min) make it perfect for creating intricate designs and thin-walled products with excellent detail.

Exceptional Strength and Durability

With 63 MPa tensile strength and 120% elongation, this resin delivers outstanding toughness and flexibility for long-lasting, impact-resistant products.

Reliable Heat and UV Performance

Features impressive heat resistance up to 148°C and UV stability, making it ideal for both indoor and outdoor applications.

WONDERLITE® PC-122U

WONDERLITE® PC-122u Datasheet

UV Stabilized PC WONDERLITE® PC-122U
Product Description: UV Stabilized
PropertiesISO Test MethodTest ConditionUnitPC-122U
Melt Flow Index1133300℃ × 1.2KGml/10 min22
Mass Density118323  ℃g/cm31.2
Tensile Strength52750 mm/min, yieldMPa63
50 mm/min, breakMPa70
Tensile Elongation52750 mm/min%120
Flexural Strength1782 mm/minMPa90
Flexural Modulus1782 mm/minGPa2.4
Izod Impact Strength180/1A23℃, Notched,1/8″KJ/m260
-30℃, Notched,1/8″KJ/m2
Charpy Impact Strength17923℃, NotchedKJ/m260
-30℃, NotchedKJ/m2
Vicat Softening Temp.30650℃/hr;1KG148
50℃/hr;5KG143
Heat Distortion Temp.75/A1.8MPa, unannealed127
1.8MPa, annealed142
Coefficient of Linear Thermal Expansion113596.0~8.0×10-5
FlammabilityUL-943.0mm V-2
Mold Shrinkage294-4%0.5~0.7
Symbol1043>PC<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

WONDERLITE® PC-122u UL Product iQ

WONDERLITE® PC-122U(f2) UL Product iQ
File Number: E56070Yellow Card™Polycarbonate (PC) “WONDERLITE”, furnished as pellets
(f2) – Subjected to one or more of the following tests: Ultraviolet Light, Water Exposure or Immersion in accordance with UL 746C, where the acceptability for outdoor use is to be determined by UL.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
0.75 mm, Color: ALLV-2
3.0 mm, Color: ALLV-2
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
0.75 mm, Color: ALLV-2
3.0 mm, Color: ALLV-2
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
0.75 mmPLC 4
3.0 mmPLC 2
High Amp Arc Ignition (HAI)UL 746A
0.75 mmPLC 1
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 2UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 2
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
0.75 mm120   °C
3.0 mm120   °C
Relative Thermal Index – Mechanical ImpactUL 746B
0.75 mm105   °C
3.0 mm105   °C
Relative Thermal Index – Mechanical StrengthUL 746B
0.75 mm120   °C
3.0 mm120   °C
PHYSICAL PROPERTIESVALUETEST METHOD
UV Exposure & Water Immersionf2UL 746C
Report Date: 2001-09-25

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top