WONDERLITE® PC-6600 Plastic Resin Flame Retardant Material
Wonderlite PC-6600 is a top-notch flame retardant plastic resin made by CHIMEI. It’s perfect for electrical appliances, offering great fire safety without harmful chemicals. This tough material comes in easy-to-use granules and resists flames even at just 1.0mm thick. It’s strong, heat-resistant, and electrical-friendly, making it ideal for everything from kitchen gadgets to power tools.
- Application: Electrical appliances
- Character: Flame Retardant grade
Download
Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides. All documents are sourced directly from manufacturers and updated regularly for accuracy.


WONDERLITE® PC-6600 Datasheet
| Flame Retardant WONDERLITE® PC-6600 | ||||
| Product Description: 1.0mm V-0,Opaque | ||||
| Properties | ISO Test Method | Test Condition | Unit | PC-6600 |
| Melt Flow Index | 1133 | 300℃ × 1.2KG | ml/10 min | 10 |
| Spiral flow | CHIMEI | 260℃,2mm, | cm | – |
| V:50%,P:50% | ||||
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.2 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 60 |
| 50 mm/min, break | MPa | 70 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 115 |
| Flexural Strength | 178 | 2 mm/min | MPa | 90 |
| Flexural Modulus | 178 | 2 mm/min | GPa | 2.3 |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 60 |
| -30℃, Notched | KJ/m2 | 15 | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 60 |
| -30℃, Notched | KJ/m2 | 15 | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 150 |
| 50℃/hr;5KG | ℃ | 145 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 125 |
| 1.8MPa, annealed | ℃ | 140 | ||
| Dielectric Constant | IEC 60250 | 1MHz | — | 3 |
| Volume Resistivity | IEC 60093 | — | Ohm X m | 3.6E+14 |
| Surface Resistivity | IEC 60093 | — | Ohm | 9.3E+14 |
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 6.7*10-5 |
| Flammability | – | UL-94 | – | 1.0mm V-0 |
| 2.0mm 5VB | ||||
| 3.0mm 5VA | ||||
| Mold Shrinkage | 294-4 | – | % | 0.4~0.6 |
| Symbol | 1043 | – | – | >PC< |
| January 12, 2024 | ||||
| Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test. | ||||
WONDERLITE® PC-6600 UL Product iQ
| WONDERLITE® PC-6600(Y)(a) UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Polycarbonate (PC) “WONDERLITE”, furnished as pellets |
| (Y) – Optional suffix; may be suffixed with one or two alphabet but except H, unconcerned with formula or constituent changed. | ||
| (a) – Ball pressure temperature is in accordance with IEC 60695-10-2 Method B. | ||
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.0 mm, Color: ALL | V-0 | |
| 1.5 mm, Color: ALL | V-0 | |
| 2.0 mm, Color: ALL | 5VB | |
| V-0 | ||
| 2.5 mm, Color: ALL | 5VA | |
| V-0 | ||
| 3.0 mm, Color: ALL | 5VA | |
| V-0 | ||
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.0 mm, Color: ALL | V-0 | |
| 1.5 mm, Color: ALL | V-0 | |
| 2.0 mm, Color: ALL | V-0 | |
| 2.5 mm, Color: ALL | V-0 | |
| 3.0 mm, Color: ALL | V-0 | |
| Flammability | IEC 60695-11-20 | |
| 2.0 mm, Color: ALL | 5VB | |
| 2.5 mm, Color: ALL | 5VA | |
| 3.0 mm, Color: ALL | 5VA | |
| Glow Wire Ignition Temperature (GWIT) | IEC 60695-2-13 | |
| 1.0 mm | 850 °C | |
| 1.5 mm | 875 °C | |
| 3.0 mm | 875 °C | |
| Glow Wire Flammability Index (GWFI) | IEC 60695-2-12 | |
| 1.0 mm | 930 °C | |
| 1.5 mm | 960 °C | |
| 3.0 mm | 960 °C | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.0 mm | PLC 3 | |
| 1.5 mm | PLC 3 | |
| 2.0 mm | PLC 2 | |
| 2.5 mm | PLC 2 | |
| 3.0 mm | PLC 0 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.0 mm | PLC 1 | |
| 1.5 mm | PLC 1 | |
| 2.0 mm | PLC 0 | |
| 2.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| Comparative Tracking Index (CTI) | PLC 2 | UL 746A |
| Dielectric Strength | 31 kV/mm | ASTM D149 |
| Volume Resistivity | 1.0E+14 ohms·cm | ASTM D257/IEC 60093 |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.0 mm | 130 °C | |
| 1.5 mm | 130 °C | |
| 2.0 mm | 130 °C | |
| 2.5 mm | 130 °C | |
| 3.0 mm | 130 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.0 mm | 120 °C | |
| 1.5 mm | 120 °C | |
| 2.0 mm | 120 °C | |
| 2.5 mm | 120 °C | |
| 3.0 mm | 120 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.0 mm | 130 °C | |
| 1.5 mm | 130 °C | |
| 2.0 mm | 130 °C | |
| 2.5 mm | 130 °C | |
| 3.0 mm | 130 °C | |
| Ball Pressure Temperature | 135 °C | |
| PHYSICAL PROPERTIES | VALUE | TEST METHOD |
| Dimensional Change | 0.0 % | ASTM D1042/ISO 2796 |
| Report Date: 2010-08 | ||
Related WONDERLITE® PC Plastics
Chimei WONDERLITE® PC-6715NF
Chimei WONDERLITE® PC-6710NF
Chimei WONDERLITE® PC-6700
Chimei WONDERLITE® PC-6715VT
Chimei WONDERLITE® PC-6600 J01
Chimei WONDERLITE® PC-681U
Chimei WONDERLITE® PC-616LS
Chimei WONDERLITE® PC-175
Chimei WONDERLITE® PC-145K
Chimei WONDERLITE® PC-122P
Chimei WONDERLITE® PC-115U
Chimei WONDERLITE® PC-115
Chimei WONDERLITE® PC-115L
Chimei WONDERLITE® PC-110P
Chimei WONDERLITE® PC-110L
Chimei WONDERLITE® PC-108U
Chimei WONDERLITE® PC-6610
Chimei WONDERLITE® PC-6710