Chimei Kibisan® PN-127 L200

Chimei Kibisan PN-127 L200 SAN resin

Chimei Kibisan® PN-127 L200 General Transparent Dark Blue

Chimei KIBISAN PN-127 L200 is a high-performance SAN resin designed for injection molding. This General SAN plastic stands out with its transparent dark blue color and heat-resistant properties, making it a versatile choice for industries needing both clarity and durability. Whether you’re crafting visually appealing products or parts that must withstand high temperatures, this resin delivers reliability and quality.

  • Application: External pen tubing/transparent parts for electrical and electronic products/fan blades
  • Character: Transparent dark blue, Heat Resistant Grade
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 17 ml/10 min
  • Mass Density: 1.06 g/cm³
  • Tensile Strength: 74 MPa (yield and break)
  • Flexural Strength: 105 MPa
  • Impact Strength: Izod 3 kJ/m², Charpy 2 kJ/m² (notched)
  • Vicat Softening Temperature: 105°C (1 kg), 104°C (5 kg)
  • Heat Distortion Temperature: 90°C (unannealed), 101°C (annealed)
  • Flammability: HB under UL-94 at 1.5 mm thickness
  • Mold Shrinkage: 0.2~0.7%

Transparency with Unique Blue Tint

It offers a see-through dark blue color, perfect for designs needing both clarity and aesthetics, like branded consumer goods.

High Heat Resistance

It withstands temperatures up to 101°C, ensuring parts maintain shape in hot environments, such as automotive or electronic components.

Robust Mechanical Strength

It features 74 MPa tensile and 105 MPa flexural strength, ideal for load-bearing parts that require durability and rigidity.

Kibisan PN-127 L200 SAN Resin

Applications

  • External Pen Tubing: Its transparency and blue tint enhance visual appeal, while heat resistance ensures durability during daily use, solving issues of aesthetic and functional wear.
  • Transparent Parts for Electrical and Electronic Products: Combines clarity for visibility with electrical insulation, addressing needs for safe, see-through components in devices.
  • Fan Blades: Offers mechanical strength and heat resistance, suitable for smaller fans, tackling challenges of durability in warmer operating conditions.
Chimei Kibisan PN-127 L200 Application

Kibisan® PN-127 L200 Datasheet

General SAN KIBISAN®  PN-127_L200
Product Description: Injection molding
PropertiesISO Test MethodTest ConditionUnitPN-127_L200
Melt Flow Index1133 220℃×10KGml/10 min17 
Mass Density1183 23 ℃g/cm31.06 
Tensile Strength527 50 mm/min, yieldMPa74 
50 mm/min, breakMPa74 
Tensile Elongation527 50 mm/min%
Flexural Strength178 2 mm/minMPa105 
Flexural Modulus2 mm/minGPa3.3 
Izod Impact Strength180/1A23℃, NotchedKJ/m2
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m2
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG105 
50℃/hr;5KG104 
Heat Distortion Temp.75/A1.8MPa, unannealed90 
1.8MPa, annealed101 
Coefficient of Linear Thermal Expansion11359 3.6~3.8*10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.2~0.7
Symbol1043 >SAN<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test

Kibisan® PN-127 L200 UL Product iQ

KIBISAN® PN-127 | UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)PLC 4UL 746A
(1.5 mm)
High Amp Arc Ignition (HAI)PLC 0UL 746A
(1.5 mm)
High Voltage Arc Tracking Rate (HVTR)PLC 0
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top