Chimei WONDERLITE PC-108U Extrusion Grade High Viscosity
Chimei Wonderlite® PC-108U is a high-viscosity, UV-stabilized extrusion-grade polycarbonate resin. Engineered for demanding outdoor applications, it combines exceptional durability, ease of processing, and weather resistance.
- Character: High viscosity; UV stabilized
- Application: Skylight Panel; Noise Barrier Wall; Corrugated Roof
Key technical data (ISO)
- Tensile Strength: 65 MPa (yield), 75 MPa (break)
- Flexural Strength: 90 MPa
- Heat Distortion Temp.: 128°C (1.8MPa)
- Flammability Rating: HB (1.5mm), V-2 (0.75mm)
- UV & Water Resistance: UL 746C f1 certified

Application
- Skylight Panels: UV resistance ensures clarity and prevents yellowing, while high impact strength safeguards against hail or debris.
- Noise Barrier Walls: Weather-resistant and durable, PC-108U reduces noise pollution in highways or industrial zones for decades.
- Corrugated Roofing: Combines thermal stability (HDT 128°C) and lightweight design (density 1.2 g/cm³) for long-lasting, energy-efficient roofs.

WONDERLITE® PC-108U Datasheet
| Extrusion PC WONDERLITE® PC-108U Product Description: High viscosity; UV stabilized; Easy release; For extrusion application | ||||
| Properties | ISO Test Method | Test Condition | Unit | PC-108U |
| Melt Flow Index | 1133 | 300℃ × 1.2KG | ml/10 min | 6.5 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.2 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 65 |
| 50 mm/min, break | MPa | 75 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 120 |
| Flexural Strength | 178 | 2 mm/min | MPa | 90 |
| Flexural Modulus | 2 mm/min | GPa | 2.4 | |
| Izod Impact Strength | 180/1A | 23℃, Notched,1/8″ | KJ/m2 | 75 |
| -30℃, Notched,1/8″ | KJ/m2 | – | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 75 |
| -30℃, Notched | KJ/m2 | – | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 150 |
| 50℃/hr;5KG | ℃ | 145 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 128 |
| 1.8MPa, annealed | ℃ | 143 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 6.0~8.0×10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB 0.75mm V2 |
| Mold Shrinkage | 294-4 | – | % | 0.5~0.7 |
| Symbol | 1043 | – | – | >PC< |
| March 11, 2024 Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test | ||||
WONDERLITE® PC-108U UL Product iQ
| WONDERLITE® PC-108U(f1) | UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Polycarbonate (PC) “WONDERLITE”, furnished as pellets |
| (f1) – Suitable for outdoor use with respect to exposure to Ultraviolet Light, Water Exposure and Immersion in accordance with UL 746C. | ||
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 0.75 to 0.83 mm, Color: ALL | V-2 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 0.75 to 0.83 mm, Color: ALL | V-2 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| Comparative Tracking Index (CTI) | PLC 2 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 3 | |
| High Voltage, Low Current Arc Resistance | PLC 6 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 0.75 to 0.83 mm | 80 °C | |
| 1.5 mm | 80 °C | |
| 3.0 mm | 80 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 0.75 to 0.83 mm | 80 °C | |
| 1.5 mm | 80 °C | |
| 3.0 mm | 80 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 0.75 to 0.83 mm | 80 °C | |
| 1.5 mm | 80 °C | |
| 3.0 mm | 80 °C | |
| PHYSICAL PROPERTIES | VALUE | TEST METHOD |
| UV Exposure & Water Immersion | f1 | UL 746C |
Related WONDERLITE® PC Plastics
Chimei WONDERLITE® PC-6715NF
Chimei WONDERLITE® PC-6710NF
Chimei WONDERLITE® PC-6700
Chimei WONDERLITE® PC-6715VT
Chimei WONDERLITE® PC-6600 J01
Chimei WONDERLITE® PC-681U
Chimei WONDERLITE® PC-616LS
Chimei WONDERLITE® PC-175
Chimei WONDERLITE® PC-145K
Chimei WONDERLITE® PC-122P
Chimei WONDERLITE® PC-115U
Chimei WONDERLITE® PC-115
Chimei WONDERLITE® PC-115L
Chimei WONDERLITE® PC-110P
Chimei WONDERLITE® PC-110L
Chimei WONDERLITE® PC-108U
Chimei WONDERLITE® PC-6610
Chimei WONDERLITE® PC-6710
Chimei WONDERLITE® PC-6600
Chimei WONDERLITE® PC-122u
Chimei WONDERLITE® PC-122
Chimei WONDERLITE® PC-115p
Chimei WONDERLITE® PC-110u
Chimei WONDERLITE® PC-110
Advanced Manufacturing