WONDERLITE® PC-115 Flame Retardant Grade Low Viscosity
Wonderlite PC-115, a low-viscosity Chimei polycarbonate resin, offers exceptional flow for precise injection molding. Ideal for industries needing durable, transparent parts, it simplifies production while ensuring strength and clarity in every application.
- Character: Low viscosity
- Application: General injection molding for stationery, external pen tubing, toys, transparent molded products
Key technical data (ISO)
- Melt flow index: 15 ml/10 min (300°C, 1.2 kg)
- Mass density: 1.2 g/cm³
- Tensile strength: 70 MPa
- Tensile elongation: 120%
- Vicat softening temp: 150°C (1 kg)
- Heat distortion temp: 143°C (annealed)
- Mold shrinkage: 0.5-0.7%
- Flammability: V-2 (2.5 mm)

Application
- General injection molding for stationery: Craft durable, lightweight pencil cases or rulers with ease.
- External pen tubing: Produce clear, tough pen barrels that look sharp and resist cracking.
- Toys: Create vibrant, unbreakable toy parts kids can enjoy for years.
- Transparent molded products: Design sleek, see-through casings or displays that stand out on shelves.

WONDERLITE® PC-115 Datasheet
| General PC WONDERLITE® PC-115 Product Description: Low viscosity | ||||
| Properties | ISO Test Method | Test Condition | Unit | PC-115 |
| Melt Flow Index | 1133 | 300℃ × 1.2KG | ml/10 min | 15 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.2 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 64 |
| 50 mm/min, break | MPa | 70 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 120 |
| Flexural Strength | 178 | 2 mm/min | MPa | 90 |
| Flexural Modulus | 2 mm/min | GPa | 2.4 | |
| Izod Impact Strength | 180/1A | 23℃, Notched,1/8″ | KJ/m2 | 70 |
| -30℃, Notched,1/8″ | KJ/m2 | – | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 70 |
| -30℃, Notched | KJ/m2 | – | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 150 |
| 50℃/hr;5KG | ℃ | 145 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 128 |
| 1.8MPa, annealed | ℃ | 143 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 6.0~8.0×10-5 |
| Flammability | – | UL-94 | – | 2.5mm V-2 |
| Mold Shrinkage | 294-4 | – | % | 0.5~0.7 |
| Symbol | 1043 | – | – | >PC< |
| March 11, 2024 Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test | ||||
WONDERLITE® PC-115 UL Product iQ
| WONDERLITE® PC-115(+) | UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Polycarbonate (PC) “WONDERLITE”, furnished as pellets |
| (+) – Indicate 0~0.5% acid scavengers. | ||
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 0.4 mm, Color: ALL | V-2 | |
| 1.5 mm, Color: ALL | V-2 | |
| 2.5 to 2.8 mm, Color: ALL | V-2 | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 0.4 mm, Color: ALL | V-2 | |
| 1.5 mm, Color: ALL | V-2 | |
| 2.5 to 2.8 mm, Color: ALL | V-2 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 0.4 mm | PLC 4 | |
| 1.5 mm | PLC 2 | |
| 2.5 to 2.8 mm | PLC 2 | |
| 3.0 mm | PLC 2 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 0.4 mm | PLC 4 | |
| 1.5 mm | PLC 4 | |
| 2.5 to 2.8 mm | PLC 3 | |
| 3.0 mm | PLC 3 | |
| Comparative Tracking Index (CTI) | PLC 2 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 2 | |
| High Voltage, Low Current Arc Resistance | PLC 6 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 0.4 mm | 80 °C | |
| 1.5 mm | 120 °C | |
| 2.5 to 2.8 mm | 120 °C | |
| 3.0 mm | 120 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 0.4 mm | 80 °C | |
| 1.5 mm | 105 °C | |
| 2.5 to 2.8 mm | 105 °C | |
| 3.0 mm | 105 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 0.4 mm | 80 °C | |
| 1.5 mm | 120 °C | |
| 2.5 to 2.8 mm | 120 °C | |
| 3.0 mm | 120 °C | |
Related WONDERLITE® PC Plastics
Chimei WONDERLITE® PC-6715NF
Chimei WONDERLITE® PC-6710NF
Chimei WONDERLITE® PC-6700
Chimei WONDERLITE® PC-6715VT
Chimei WONDERLITE® PC-6600 J01
Chimei WONDERLITE® PC-681U
Chimei WONDERLITE® PC-616LS
Chimei WONDERLITE® PC-175
Chimei WONDERLITE® PC-145K
Chimei WONDERLITE® PC-122P
Chimei WONDERLITE® PC-115U
Chimei WONDERLITE® PC-115
Chimei WONDERLITE® PC-115L
Chimei WONDERLITE® PC-110P
Chimei WONDERLITE® PC-110L
Chimei WONDERLITE® PC-108U
Chimei WONDERLITE® PC-6610
Chimei WONDERLITE® PC-6710
Chimei WONDERLITE® PC-6600
Chimei WONDERLITE® PC-122u
Chimei WONDERLITE® PC-122
Chimei WONDERLITE® PC-115p
Chimei WONDERLITE® PC-110u
Chimei WONDERLITE® PC-110
Advanced Manufacturing