Chimei WONDERLITE® PC-6710NF

Chimei Wonderlite PC-6710NF PC Resin

Chimei WONDERLITE PC-6710NF Flame Retardant Grade Transparent

WONDERLITE® PC-6710NF is a high-performance, PFAS-free flame-retardant polycarbonate resin offering UL 94 V-0 compliance at 3.0 mm thickness. With exceptional transparency, UV stability, and robust mechanical strength, it’s engineered for industries prioritizing safety, durability, and regulatory compliance.

  • Character: Transparent, Flame retardant (PFAS Free), 3.0 mm V0
  • Application: Electrical appliances, outdoor applications (UL 746C f1)
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Flame Retardancy: UL 94 V-0 (3.0 mm), IEC 60695-11-10 V-0, PFAS-free.
  • Mechanical Strength: Tensile Strength 65 MPa, Flexural Modulus 2.3 GPa.
  • Thermal Performance: HDT 125°C (unannealed), Vicat Softening 148°C.
  • Electrical Safety: Dielectric Strength 24 kV/mm, CTI PLC 4.
  • Impact Resistance: 65 KJ/m² (Charpy, 23°C).
  • Certifications: UL Recognized (E56070), RoHS compliant.

Superior Flame Resistance, PFAS-Free

WONDERLITE® PC-6710NF meets UL 94 V-0 standards (3.0 mm) without harmful PFAS chemicals. Ideal for electrical enclosures or automotive interiors where safety and eco-compliance matter.

High Impact & Thermal Stability

It boasts 65 KJ/m² Charpy impact resistance (23°C) and a Vicat softening temperature of 148°C. Perfect for outdoor equipment or medical devices exposed to harsh conditions.

UL-Certified Outdoor Durability

UV-stabilized and UL 746C f1-rated for outdoor use. Protects components like LED housings or solar connectors from weathering and electrical stress.

Wonderlite® PC-6710NF

Application

  • Electrical Appliances: Circuit breakers, switchgear, and connectors requiring flame resistance.
  • Outdoor Infrastructure: Solar panel junction boxes, LED streetlight housings (UL 746C f1 compliant).
  • Medical Devices: Sterilizable equipment housings needing clarity and durability.
  • Transportation: Automotive charging ports or battery covers demanding thermal stability.
Chimei Wonderlite PC-6710NF Application

WONDERLITE® PC-6710NF Datasheet

Flame Retardant PC WONDERLITE®  PC-6710NF (Provisional)   
Product Description: 3.0mm V-0,PFAS free, UV Stabilized,Transparent
PropertiesISO Test MethodTest ConditionUnitPC-6710NF
Melt Flow Index1133 300℃  ×  1.2KGml/10 min10 
Spiral flowCHIMEI260℃,2mm,
V:50%,P:50%
cm
Mass Density1183 23  ℃g/cm31.2 
Tensile Strength527 50 mm/min, yieldMPa65 
50 mm/min, breakMPa70 
Tensile Elongation527 50 mm/min%110 
Flexural Strength178 2 mm/minMPa95 
Flexural Modulus2 mm/minGPa2.3 
Izod Impact Strength180/1A23℃, NotchedKJ/m260 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m265 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG148 
50℃/hr;5KG142 
Heat Distortion Temp.75/A1.8MPa, unannealed125 
1.8MPa, annealed140 
Dielectric ConstantIEC 602501MHz
Volume ResistivityIEC 60093Ohm X m1E+16
Surface ResistivityIEC 60093Ohm1E+16
Coefficient of Linear Thermal Expansion11359 6.8*10-5
FlammabilityUL-943.0mm V-0
Mold Shrinkage294-4%0.4~0.6
Symbol1043 >PC<
August 2, 2024
Notes: These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

WONDERLITE® PC-6710NF UL Product iQ

WONDERLITE® PC-6710NF | UL Product iQ
File Number: E56070Yellow Card™Polycarbonate (PC) “WONDERLITE”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityV-0ANSI/UL 94
(3.0 to 3.3 mm, Color: NC)
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityV-0IEC 60695-11-10
(3.0 to 3.3 mm, Color: NC)
Glow Wire Ignition Temperature (GWIT)825   °CIEC 60695-2-13
(3.0 to 3.3 mm)
Glow Wire Flammability Index (GWFI)960   °CIEC 60695-2-12
(3.0 to 3.3 mm)
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)PLC 3UL 746A
(3.0 to 3.3 mm)
High Amp Arc Ignition (HAI)PLC 2UL 746A
(3.0 to 3.3 mm)
Comparative Tracking Index (CTI)PLC 4UL 746A
Dielectric Strength24   kV/mmASTM D149
High Voltage Arc Tracking Rate (HVTR)PLC 3
Volume Resistivity1.0E+15   ohms·cmASTM D257/IEC 60093
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical Strength80   °CUL 746B
(3.0 to 3.3 mm)
Relative Thermal Index – Mechanical Impact80   °CUL 746B
(3.0 to 3.3 mm)
Relative Thermal Index – Mechanical Strength80   °CUL 746B
(3.0 to 3.3 mm)
Ball Pressure Temperature135   °C
PHYSICAL PROPERTIESVALUETEST METHOD
Dimensional Change0.0   %ASTM D1042/ISO 2796

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top