WONDERLITE PC-6715NF Flame Retardant Grade Transparent

The WONDERLITE® PC-6715NF is a transparent, PFAS-free polycarbonate resin offering UL 94 V-0 flame retardancy at 1.5mm thickness. Engineered for safety and durability, it combines UV stabilization, high impact resistance, and compliance with global electrical/thermal standards—ideal for railways, appliances, and outdoor applications.

  • Character: Transparent, Flame retardant (PFAS Free), 1.5 mm V0
  • Application: Railway, Electrical appliances, outdoor applications
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Flame Retardancy: UL 94 V-0 (1.5mm–3.0mm thickness), PFAS-free.
  • Vicat Softening Temp: 150°C
  • Heat Distortion Temp (1.8MPa): 125°C
  • Tensile Strength: 60 MPa (yield)
  • Flexural Strength: 99 MPa
  • Impact Resistance: 60 KJ/m² (Izod/Charpy at 23°C)
  • Volume Resistivity: 1E+16 Ω·m
  • Dielectric Strength: 24 kV/mm
  • Melt Flow Index: 5 ml/10min (300°C)
  • Mold Shrinkage: 0.4–0.6%

PFAS-Free Flame Retardancy

WONDERLITE® PC-6715NF meets UL 94 V-0 flammability standards without hazardous PFAS chemicals. This ensures compliance with strict safety regulations, making it perfect for electrical enclosures and public infrastructure where fire safety is critical.

UV Resistance for Outdoor Durability

UV-stabilized to resist yellowing and degradation, this material maintains clarity and strength in harsh sunlight. Use it for outdoor lighting covers, traffic signs, or railway components exposed to weather.

High Impact Strength

With 60 KJ/m² Izod impact resistance at 23°C, PC-6715NF withstands sudden shocks and vibrations. Ideal for automotive interiors, appliance housings, or protective covers in demanding environments.

Wonderlite®-PC-6715NF

Application

  • Railway: Seat components, cabin panels, and lighting covers requiring flame retardancy and impact resistance.
  • Electrical Appliances: Connectors, circuit breaker housings, and enclosures needing UL-certified safety.
  • Outdoor Applications: UV-resistant traffic signs, LED streetlight covers, and solar panel frames.
Chimei-Wonderlite-PC-6715NF-Application

WONDERLITE® PC-6715NF Datasheet

Flame Retardant WONDERLITE®  PC-6715NF (Provisional)
Product Description: 1.5mm V-0,PFAS free,UV Stabilized,Transparent
PropertiesISO Test MethodTest ConditionUnitPC-6715NF
Melt Flow Index1133 300℃  ×  1.2KGml/10
min
Spiral flowCHIMEI260
℃,2mm,V:50%,P:50%
cm
Mass Density1183 23 ℃g/cm31.2 
Tensile Strength527 50 mm/min, yieldMPa60 
50 mm/min, breakMPa55 
Tensile Elongation527 50 mm/min%70 
Flexural Strength178 2 mm/minMPa99 
Flexural Modulus2 mm/minGPa2.2 
Izod Impact Strength180/1A23℃, NotchedKJ/m260 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m260 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG150 
50℃/hr;5KG143 
Heat Distortion Temp.75/A1.8MPa, unannealed125 
Dielectric ConstantIEC 602501MHz
Volume ResistivityIEC 60093Ohm
X m
1E+16
Surface ResistivityIEC 60093Ohm1E+16
Coefficient of Linear Thermal
Expansion
11359 6.8*10-5
FlammabilityUL-941.5mm V-0
Mold Shrinkage294-4%0.4~0.6
Symbol1043 >PC<
August 2, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test

WONDERLITE® PC-6715NF UL Product iQ

WONDERLITE® PC-6715NF(a) | UL Product iQ
File Number: E56070Yellow Card™Polycarbonate (PC) “WONDERLITE”, furnished as pellets
(a) – Ball pressure temperature is in accordance with IEC 60695-10-2 Method B.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: NC, BKV-0
2.0 mm, Color: NC, BKV-0
3.0 mm, Color: NC, BKV-0
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: NC, BKV-0
2.0 mm, Color: NC, BKV-0
3.0 mm, Color: NC, BKV-0
Glow Wire Ignition Temperature (GWIT)IEC 60695-2-13
1.5 mm875   °C
3.0 mm875   °C
Glow Wire Flammability Index (GWFI)IEC 60695-2-12
1.5 mm960   °C
3.0 mm960   °C
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
2.0 mmPLC 4
3.0 mmPLC 2
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 2
2.0 mmPLC 2
3.0 mmPLC 2
Comparative Tracking Index (CTI)PLC 4UL 746A
Dielectric Strength24   kV/mmASTM D149
High Voltage Arc Tracking Rate (HVTR)PLC 3
Volume Resistivity1.0E+16   ohms·cmASTM D257/IEC 60093
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm80   °C
2.0 mm80   °C
3.0 mm80   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm80   °C
2.0 mm80   °C
3.0 mm80   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm80   °C
2.0 mm80   °C
3.0 mm80   °C
Ball Pressure Temperature135   °C
PHYSICAL PROPERTIESVALUETEST METHOD
Dimensional Change0.0   %ASTM D1042/ISO 2796

Related WONDERLITE® PC Plastics

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top