LG Chem ABS SG175G

LG Chem ABS Resin

LG ABS SG175G General Grade

LG ABS SG175G is a premium injection molding ABS resin engineered for exceptional high gloss and superior flow, making it ideal for high-quality surface finishes and complex part designs.

  • Character: Super Gloss, High Flow.
  • Application: Electrical/Electronic Products
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Melt Flow Index (220°C, 10kg): 36 g/10min
  • Tensile Strength at Yield: 44 MPa
  • Flexural Modulus: 2500 MPa
  • Izod Impact Strength (Notched, 3.2mm): 250 J/m
  • Heat Deflection Temperature (1.82MPa): 85°C
  • Specific Gravity: 1.05
  • Mold Shrinkage: 0.4–0.7%

Application

  • Electrical enclosures and housings
  • Consumer electronics components
  • Automotive interior trim parts
  • Household appliance surfaces
  • High-gloss decorative items

Features & Benefits

Exceptional Surface Gloss

It delivers a brilliant, mirror-like finish that enhances product aesthetics without additional post-processing, perfect for consumer-facing components.

High Fluidity for Complex Molds

It ensures easy filling of intricate mold designs, reducing injection pressure and cycle time while minimizing defects like short shots or weld lines.

Balanced Mechanical Properties

It offers strong impact resistance and rigidity, providing durability and structural integrity for functional parts in demanding applications.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturingg

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top