LG Chem ABS AF312B

LG Chem ABS Resin

LG ABS AF312B Flame Retardant Grade

LG ABS AF312B from LG Chem is a high-flow, flame-retardant ABS resin ideal for injection molding. It achieves a superior V-0 rating at just 2.1mm thickness, making it a reliable and efficient material choice for demanding electrical and consumer appliance components.

  • Character: Fire resistance (2.1mm V-0). Opaqueness, Hot Stamping, Paintability, High Gloss, Dimensional Stability, High Flow.
  • Application: Heater, electric control box, Charge bank, hair dryer.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Melt Flow Rate (220°C / 10.0 kg): 55 g/10min
  • Tensile Strength at Yield: 42 MPa
  • Flexural Modulus: 2250 MPa
  • Izod Impact Strength (Notched): 21 J/m
  • Heat Deflection Temperature (HDT @ 1.82 MPa): 74 °C
  • Rockwell Hardness (R-Scale): 100
  • Specific Gravity: 1.15 g/cm³
  • Flame Retardancy: UL94 V-0 @ 2.1mm
  • Drying: 70-80°C for 2-4 hours
  • Melt Temperature: 190-230°C
  • Mold Temperature: 40-70°C
  • Fully compliant with EU RoHS

Application

  • Heaters and heating appliance housings
  • Electric control boxes and enclosures
  • Charge banks and power storage units
  • Hair dryers and other personal care appliances

Features & Benefits

Superior Flame Retardant Performance

LG ABS AF312B delivers a UL94 V-0 rating at 2.1mm, ensuring critical safety compliance for electronic enclosures and components, reducing fire risks in end-use applications.

Exceptional High-Flow Processing

With a melt flow of 55 g/10min, this material fills complex molds easily, enabling faster cycle times, higher production efficiency, and excellent replication of intricate part details.

RoHS Compliant & Reliable Quality

Certified free of restricted substances, this LG Chem resin ensures your products meet global environmental regulations, simplifying your supply chain and compliance verification.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity