LG Chem ABS AF362H

LG Chem ABS Resin

LG ABS AF362H Flame Retardant Grade

LG ABS AF362H is a flame-retardant ABS resin designed for injection molding. It offers superior V-0 flammability rating at 2.5mm, high thermal resistance, and excellent stability for demanding applications.

  • Character: fire resistance (3.2mm V-0)
  • Application: Blood pressure monitor, oxygen concentrator, pulse monitor
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Flame Retardancy (UL94): V-0 @ 2.5mm thickness
  • Melt Flow Index: 55 g/10min (220°C / 10.0 kg)
  • Heat Deflection Temp. (HDT): 84.0°C @ 1.82 MPa
  • Flexural Strength: 65 MPa
  • Flexural Modulus: 2400 MPa
  • Izod Impact Strength: 22 J/m (Notched)
  • Specific Gravity: 1.15
  • RoHS Compliance: Fully Compliant (SGS Certified)
  • Form: Opaque White Pellets

Application

  • Blood Pressure Monitors
  • Oxygen Concentrators
  • Pulse Monitors

Features & Benefits

Superior Flame Retardant Safety

It achieves a UL94 V-0 rating at 2.5mm thickness, ensuring critical fire safety for sensitive electronic and medical device components, protecting both users and equipment.

Excellent Thermal Resistance

With a Heat Deflection Temperature of 84°C, this ABS resin maintains structural integrity when exposed to heat, ensuring reliable performance in enclosed environments.

High Flow for Easy Processing

A high melt flow index (55 g/10min) allows for easy filling of complex and thin-walled molds, reducing cycle times and improving manufacturing efficiency.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top