LG Chem ABS AF365F-L

LG Chem ABS Resin

LG ABS AF365F-L Flame Retardant Grade

LG ABS AF365F-L is a flame-retardant ABS resin engineered for injection molding. It achieves a superior V-0 rating at just 2.0mm thickness, offering exceptional high flow for easy processing and excellent dimensional stability for reliable part performance.

  • Character: Flame Retardancy, Dimensional Stability, High Flow
  • Application: Television, Bidet, Electrical/Electronic Products
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ASTM)

  • Flammability (UL 94): V-0 @ 2.0mm, 2.5mm, 3.0mm | V-1 @ 1.7mm
  • Relative Density: 1.16
  • Melt Flow Index (220°C/10kg): 55 g/10min
  • Tensile Strength at Yield: 41 MPa
  • Flexural Modulus: 2350 MPa
  • Izod Impact (Notched, 3.2mm): 200 J/m
  • Heat Deflection Temp (1.82MPa): 84 °C
  • Comparative Tracking Index (CTI): PLC 2
  • Relative Thermal Index (RTI Elec): 85 °C
  • RoHS & REACH: Fully Compliant

Application

  • Blood Pressure Monitors
  • Oxygen Concentrators
  • Pulse Monitors

Features & Benefits

Superior Flame Retardant Performance

This material meets strict UL 94 V-0 and 5VA standards, ensuring critical safety compliance for electronic enclosures and components, reducing fire risk in end-use applications.

Excellent High Flow Properties

Its high fluidity allows for easy filling of complex and thin-walled molds, resulting in fewer defects, higher production efficiency, and lower energy consumption during processing.

Reliable Dimensional Stability

Parts maintain their shape and size under various conditions, ensuring precise fit and long-term performance, which is crucial for assemblies and components with tight tolerances.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Raw Material Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity