LG Chem ABS TR552F

LG Chem ABS Resin

LG ABS TR552F Transparent Grade

LG ABS TR552F is a premium transparent MABS resin engineered for injection molding and extrusion. It delivers an exceptional balance of high optical clarity, superior resistance to whitening, and excellent impact strength for demanding applications.

  • Character:
  • Application:
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ASTM)

  • Melt Flow Index (220°C/10 kg): 5 g/10min
  • Tensile Strength at Yield: 40 MPa
  • Notched Izod Impact (23°C, 3.2mm): 50 J/m
  • Flexural Modulus: 1700 MPa
  • Heat Deflection Temp (1.82 MPa, Unannealed): 79 °C
  • Light Transmittance (3.2mm): 91%
  • Specific Gravity: 1.05
  • RoHS & Phthalates Compliance: Fully compliant

Application

  • Artificial Nails
  • Edge Banding

Features & Benefits

Exceptional Optical Clarity

It experience crystal-clear transparency with high light transmittance, ideal for products where visual appeal and seeing internal components are critical.

Superior Whitening Resistance

It maintains its pristine clarity and resists stress whitening after bending or impact, ensuring a lasting high-quality finish and product durability.

High Impact Strength & Softness

It offers reliable toughness and a degree of flexibility at various temperatures, providing excellent durability and a premium, soft-touch feel.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top