LG ABS TR557 Transparent Grade

LG ABS TR557 is a premium transparent ABS resin engineered for injection molding. It delivers an exceptional balance of high impact strength and outstanding optical clarity, making it ideal for demanding consumer and industrial applications.

  • Character: Transparency, High Impact Strength
  • Application: Washing Machine, Refrigerator, Electrical/Electronic Products, Miscellaneous Goods.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Specific Gravity: 1.09
  • Melt Flow Index (220°C/10kg): 23 g/10min
  • Tensile Strength at Yield: 48 MPa
  • Flexural Strength: 71 MPa
  • Izod Impact Strength (Notched, 3.2mm): 170 J/m
  • Heat Deflection Temp (1.82 MPa, Unannealed): 81 °C
  • Vicat Softening Temperature: 89 °C
  • Luminous Transmittance (3.2mm): 90%
  • Haze: 1.5%
  • Flammability Rating (UL94): HB (1.5mm & 3.0mm)
  • Relative Thermal Index (RTI Elec): 50.0 °C
  • RoHS & Phthalate-Free (Compliant per testing)

Application

  • Washing Machine: For transparent lids, detergent dispensers, and control panel covers.
  • Refrigerator: For durable and clear vegetable drawers, interior trim, and door handles.
  • Electrical/Electronic Products: For protective covers, housings for displays, and transparent structural components.
  • Miscellaneous Goods: For a variety of consumer goods requiring a tough, transparent plastic, such as cosmetic cases, office supplies, and home appliances.

Features & Benefits

Exceptional Optical Clarity

TR557 offers high luminous transmittance (90%) and low haze (1.5%), providing crystal-clear visibility for components where aesthetics and display functionality are critical.

Superior Impact Resistance

This material maintains high impact strength (170 J/m at 23°C) even at low temperatures, ensuring product durability and reducing the risk of failure from physical shocks.

Excellent Processing Versatility

With a wide processing window (200-250°C) and good melt flow, TR557 ensures easy molding, high production efficiency, and excellent replication of complex part details.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top