LG ABS XR401B Heat Resistant Grade
LG ABS XR401B is a high-performance ABS resin engineered for injection molding. It delivers an exceptional balance of high heat resistance, superior paintability, and strong chemical resistance, making it a reliable choice for demanding applications.
- Character: High Heat Resistance, Paintability, Chemical Resistance
- Application: Automotive Interior Parts, Consumer Appliances, Painted Consumer Electronics, General Industrial Parts
Key technical data
- Tensile Strength at Yield: 52 MPa
- Flexural Modulus: 2600 MPa
- Izod Impact Strength (Notched, 23°C, 3.2mm): 190 J/m
- Heat Deflection Temperature (HDT) @ 1.82 MPa: 97°C
- Heat Deflection Temperature (HDT) @ 0.46 MPa: 105°C
- Vicat Softening Temperature: 106°C
- Melt Flow Index (220°C/10kg): 11 g/10min
- Specific Gravity: 1.05
- Mold Shrinkage: 0.4 – 0.7%
- Drying: 80-90°C for 3-4 hours
- Melt Temperature: 220-290°C
- Mold Temperature: 40-80°C
Application
- Automotive Interior Parts
- Consumer Appliances
- Painted Consumer Electronics
- General Industrial Parts
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR630
LG Chem ABS XR474
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
Advanced Manufacturing