LG Chem ABS XR404T

LG Chem ABS Resin

LG ABS XR404T Heat Resistant Grade

LG ABS XR404T is a high-performance ABS resin engineered specifically for rear combination lamp housings. It delivers exceptional welding strength with PMMA lenses, superior surface quality, and high heat resistance for demanding automotive applications.

  • Character: High Heat Resistance, Welding, Superior Surface Quality, Welding Strength
  • Application: Rear Combination Lamp
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Heat Deflection Temperature (HDT): 102°C @ 1.82 MPa
  • Izod Impact Strength (Notched): 180 J/m @ 23°C
  • Tensile Strength at Yield: 53 MPa
  • Melt Flow Index (MFI): 6.5 g/10min (220°C/10kg)
  • Flammability Rating (UL 94): HB @ 3.0mm
  • Specific Gravity: 1.05
  • Drying: 80-90°C for 3-4 hours
  • Melt Temperature: 230-270°C
  • Mold Temperature: 40-80°C

Application

  • Rear Combination Lamp Housings

Features & Benefits

Superior Heat Resistance

With a Heat Deflection Temperature of 102°C, this ABS XR404T LG Chem material withstands the high temperatures near car engines and lights, preventing deformation and ensuring long-term reliability.

Excellent Impact Strength

It offers high Izod impact strength (180 J/m), making components durable and resistant to cracking during assembly, handling, or from road debris, which reduces breakage and warranty claims.

High Welding Strength with PMMA

Specifically formulated for strong welding bonds with PMMA lenses, this LG ABS XR404T ensures leak-proof and secure lamp assemblies, streamlining your production process with reliable results.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity