LG Chem ABS XR410

LG Chem ABS Resin

LG ABS XR410 Heat Resistant Grade

LG ABS XR410 from LG Chem is a high-heat ABS resin engineered for interior parts. It features low gloss, very low VOC emissions, and does not require painting, simplifying your manufacturing process.

  • Character: High Heat Resistance, Non Painting, Low TVOC, Low Gloss
  • Application: Cockpit, Door Trim, Interior ETC
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Heat Deflection Temperature (HDT @ 1.82 MPa, Annealed): 103 °C
  • Heat Deflection Temperature (HDT @ 0.46 MPa, Annealed): 108 °C
  • Vicat Softening Temperature: 107 °C
  • Tensile Strength: 48 MPa
  • Flexural Modulus: 2400 MPa
  • Izod Impact (Notched, 23°C): 155 J/m
  • UL 94 Rating (1.5mm & 3.0mm): HB
  • Drying Temperature: 80 – 90 °C
  • Melt Flow Index: 7 g/10min

Application

  • Cockpit Modules & Instrument Panels
  • Door Trims and Interior Handles
  • Various Interior Trim Components

Features & Benefits

Exceptional Heat Resistance

With a Heat Deflection Temperature up to 108°C, XR410 maintains its shape and strength in high-temperature environments, such as car interiors under direct sunlight, ensuring long-term part reliability.

Low VOC for Healthier Interiors

This material is formulated for minimal Total Volatile Organic Compound (TVOC) emission. It helps you meet stringent indoor air quality standards for automotive cabins, creating a safer and more comfortable environment.

Ready-to-Use Low Gloss Finish

XR410 provides a consistent, non-reflective low-gloss surface directly out of the mold. This eliminates the need for secondary painting, reducing production costs and time for parts like dashboards and trim.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top