LG ABS XR470 Heat Resistant Grade
LG ABS XR470 is an advanced ABS resin engineered for high-heat interior components. It combines ultra-high heat resistance with low VOC emissions and a low-gloss finish, making it ideal for demanding automotive applications where performance and interior air quality are critical.
- Character: Ultra High Heat Resistance, Low TVOC
- Application: Cockpit, Door Trim, Others
Key technical data
- Heat Deflection Temperature (HDT): 112 °C (@1.82 MPa)
- Vicat Softening Temperature: 121 °C
- Izod Impact Strength (Notched): 110 J/m (6.4mm thickness)
- Flexural Modulus: 2,500 MPa
- Tensile Strength at Yield: 45 MPa
- Melt Flow Index: 2 g/10min (220°C/10kg)
- Specific Gravity: 1.07
Application
- Cockpit Modules (e.g., dashboard skeletons, instrument clusters)
- Door Trim Panels and interior hardware
- Other Automotive Interior Parts requiring high heat and low gloss
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
LG Chem ABS ER232
LG Chem ABS BM662
LG Chem ABS XG571-G
Advanced Manufacturing