LG Chem ABS XR474

LG Chem ABS Resin

LG ABS XR474 Heat Resistant Grade

LG ABS XR474 is an ultra-high heat ABS resin with low gloss and low VOC emissions. It is engineered for high-performance, non-painted interior and exterior parts, offering exceptional durability and compliance.

  • Character: Ultra High Heat Resistance, Non Painting, Low TVOC
  • Application: Automotive Interior & Exterior Parts, Consumer Electronics Housings
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Heat Deflection Temperature (HDT @ 1.82 MPa): 112 °C – 118 °C
  • Vicat Softening Temperature: 122 °C
  • Tensile Strength: 47 MPa
  • Flexural Modulus: 2450 MPa
  • Izod Impact (Notched, 23°C): 135 J/m
  • UL94 Rating (1.5mm & 3.0mm): HB
  • Melt Flow Index (220°C/10kg): 3 g/10min
  • Drying Conditions: 80-90°C for 3-4 hours

Application

  • Automotive Interior Parts (e.g., dashboard components, trim panels)
  • Automotive Exterior Parts (e.g., grilles, mirror housings)
  • Consumer Electronics Housings
  • Household Appliances
  • Office Equipment

Features & Benefits

Ultra-High Heat Resistance

With a Heat Deflection Temperature up to 123°C, LG ABS XR474 withstands extreme thermal conditions, preventing deformation in hot environments and ensuring long-term part reliability.

Low VOC for Interior Safety

This ABS XR474 LG Chem grade features very low VOC content, contributing to better indoor air quality and meeting stringent emission standards for automotive interiors and enclosed spaces.

Inherent Low-Gloss & Toughness

The material provides a consistent low-gloss surface directly from the mold and high impact strength, eliminating the need for painting and reducing costs while ensuring durable, scratch-resistant parts.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top