LG ABS XR490 Heat Resistant Grade
LG ABS XR490 is a high-heat ABS resin engineered for automotive interiors. It delivers ultra-high heat resistance, a low-gloss non-paint surface, and very low VOC emissions for enhanced in-cabin air quality.
- Character: Ultra High Heat Resistance, Non Painting, Low TVOC, Low Gloss
- Application: Cockpit, Door Trim, Others
Key technical data
- Heat Deflection Temperature (HDT): 106 °C (@1.82 MPa)
- Vicat Softening Temperature: 115 °C
- Tensile Strength at Yield: 49 MPa
- Izod Impact Strength (Notched, 23°C): 135 J/m
- Flexural Modulus: 2500 MPa
- Melt Flow Index (220°C/10kg): 3 g/10min
- Specific Gravity: 1.07
- Mold Shrinkage: 0.4 – 0.7 %
- Rockwell Hardness (R-Scale): 113
Application
- Cockpit Modules & Instrument Panels
- Door Trim Panels
- Console Boxes
- Glove Compartments
- Trunk Trim
- Seat Belt Buckles
Features & Benefits

Related LG ABS Resin Products
LG Chem ABS XR490
LG Chem ABS XR470
LG Chem ABS XR440
LG Chem ABS XR438
LG Chem ABS XR410
LG Chem ABS XR409H
LG Chem ABS XR404T
LG Chem ABS XR404
LG Chem ABS XR401
LG Chem ABS XR401B
LG Chem ABS NF424
LG Chem ABS ER468
LG Chem ABS ER460
LG Chem ABS ER400-M
LG Chem ABS ER400-C
LG Chem ABS ER400
LG Chem ABS ER232
LG Chem ABS BM662
Advanced Manufacturing