LG Chem ABS XR630

LG Chem ABS Resin

LG ABS XR630 Heat Resistant Grade

LG ABS XR630 by LG Chem is a heat-resistant extrusion-grade ABS resin. It offers exceptional resistance to cleaning agents and high temperatures, making it ideal for demanding industrial profiles and components.

  • Character: High Heat Resistance, Chemical Resistance
  • Application: Window Profile Insulation Bar
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Heat Deflection Temperature (HDT): 102°C @ 1.82 MPa
  • Tensile Strength at Yield: 42 MPa
  • Flexural Modulus: 2150 MPa
  • Izod Impact Strength (Notched): 310 J/m (3.2mm)
  • Melt Flow Index (MFI): 2.5 g/10min (220°C/10kg)
  • Specific Gravity: 1.06

Application

  • Window Profile Insulation Bar

Features & Benefits

Excellent High Heat Resistance

With a Heat Deflection Temperature of up to 102°C, XR630 maintains structural integrity in high-temperature environments, preventing deformation and ensuring long-term product reliability.

Superior Chemical Resistance

This material is specifically designed to withstand harsh cleaning agents, making it perfect for applications requiring frequent cleaning or exposure to chemicals without degrading.

Robust Mechanical Strength

XR630 provides strong tensile and flexural strength, along with good impact resistance, resulting in durable and reliable end-products that can withstand physical stress.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top