CYCOLOY™ Resin C4210HF

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy C4210HF (PC/ABS) Resin

Cycoloy Resin C4210HF C4210HF is a 10% glass-reinforced PC+ABS blend. It delivers an exceptional balance of high flow for easy processing, high heat resistance for durability, and superior strength with good impact and appearance.

  • Character: excellent flow/impact/high heat resistance. Low temperature ductility
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength (Yield): 90 MPa
  • Flexural Modulus: 4250 MPa
  • Izod Impact (Notched): 8 kJ/m²
  • Heat Deflection Temp (HDT/A @1.8 MPa): 123 °C
  • Vicat Softening Temperature (B/120): 136 °C
  • Relative Temperature Index (RTI): 60 °C
  • Physical & Processing Properties
  • Melt Volume Rate (260°C/5kg): 33 cm³/10 min
  • Mold Shrinkage: 0.3 – 0.5 %
  • Density: 1.22 g/cm³
  • Volume Resistivity: >1E+15 Ω·cm

Application

  • Automotive Interior & Exterior Parts
  • Electrical Enclosures & Housings
  • Consumer Electronics Housings
  • Industrial Components

Features & Benefits

Enhanced Flow for Complex Molding

The high flow rate of Cycoloy C4210HF PC+ABS fills intricate molds effortlessly, reducing cycle times and minimizing defects for higher productivity and lower part costs.

Withstands High-Temperature Environments

With a Heat Deflection Temperature of 123°C at 1.8 MPa, this material maintains its structural integrity in demanding applications, ensuring reliability and long-term performance.

Superior Strength and Rigidity

The 10% glass reinforcement provides excellent stiffness and strength, allowing for the design of thin-walled yet durable components that resist deformation under load.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity