CYCOLOY™ Resin C4220

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy C4220 (PC/ABS) Resin

Cycoloy Resin C4220 Resin C4220 is a high-performance PC+ABS blend reinforced with 20% glass. It delivers an exceptional balance of high heat resistance, superior strength, and rigidity, alongside good impact strength and surface appearance for demanding engineering applications.

  • Character: with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength (Yield): 90 MPa
  • Tensile Modulus: 6,000 MPa
  • Flexural Modulus: 5,300 MPa
  • Izod Impact (Notched): 8 kJ/m²
  • Heat Deflection Temp (HDT/A @1.8 MPa): 129 °C
  • Vicat Softening Temperature (B/120): 137 °C
  • Melt Volume Rate (260°C/5.0 kg): 12 cm³/10 min
  • Density: 1.3 g/cm³
  • Mold Shrinkage (Flow): 0.2 – 0.4 %

Application

  • Automotive Components: Interior trim, brackets, and under-hood parts requiring heat resistance.
  • Electrical Enclosures: Housings for power tools, industrial controls, and connectors.
  • Consumer Appliances: Housings for kitchen devices, power tool bodies, and structural parts.
  • Industrial Components: Machine housings, covers, and parts requiring stiffness and durability.

Features & Benefits

Enhanced Heat Resistance & Stability

With a Heat Deflection Temperature of 129°C at 1.8 MPa, this Cycoloy C4220 PC+ABS maintains structural integrity in high-temperature environments, preventing deformation and ensuring long-term reliability.

Superior Strength and Rigidity

The 20% glass reinforcement provides a high tensile modulus of 6000 MPa, offering excellent stiffness and load-bearing capacity for parts that must resist bending and withstand significant mechanical stress.

Reliable Impact and Electrical Performance

This material provides good notched impact strength and high volume resistivity (>1.E+15 Ω·cm), making it a safe and durable choice for components that require both mechanical toughness and reliable electrical insulation.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top