CYCOLOY™ Resin CM8622

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy CM8622 (PC/ABS) Resin

Cycoloy Resin CM8622 is a high-heat PC/ABS blend engineered for superior strength, dimensional stability, and excellent impact resistance, ideal for demanding applications.

  • Character: with 20% Glass Reinforce. High heat resistance; Excellent balance strength/rigidity; Good impact/appearance.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 47 MPa
  • Flexural Modulus: 3,650 MPa
  • Izod Impact (Notched): 250 J/m at 23°C
  • Heat Deflection Temp (HDT): 112°C @ 1.82 MPa
  • Vicat Softening Temperature: 133°C (ISO 306)
  • Melt Flow Rate: 16 g/10 min (260°C/5.0 kgf)
  • Specific Gravity: 1.25
  • Processing (Injection Molding)
  • Melt Temperature: 270 – 300 °C
  • Mold Temperature: 60 – 100 °C
  • Drying: 2-6 hours at 110-120 °C

Application

  • Automotive Interior Components (e.g., dashboard supports, trim)
  • Consumer Electronics Housings
  • Electrical Enclosures and Connectors
  • Industrial Machine Parts
  • Durable Consumer and Telecom Devices

Features & Benefits

Exceptional Heat Resistance

With a Heat Deflection Temperature of 112°C, CYCOLOY CM8622 Resin maintains its structural integrity in high-temperature environments, ensuring reliable performance.

High Strength & Stiffness

This material offers a high flexural modulus, providing the rigidity needed for durable components that resist bending or deformation under load.

Superior Impact & Aesthetics

It delivers excellent impact strength and a superior surface finish, combining toughness with an attractive appearance right out of the mold.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity