CYCOLOY™ Resin CM8823

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy CM8823 (PC/ABS) Resin

Cycoloy Resins CM8823 is a high-heat PC/ABS blend engineered for injection molding. It delivers an exceptional balance of strength, dimensional stability, and impact resistance for demanding applications.

  • Character: high heat grade offering high modulus, low CTE, good practical impact and aesthetics.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Stress at Yield: 55 MPa
  • Flexural Modulus: 4600 MPa
  • Notched Izod Impact (+23°C): 6 kJ/m²
  • Heat Deflection Temp (HDT) @ 1.8 MPa: 118°C
  • Vicat Softening Temperature: 136°C
  • Coefficient of Thermal Expansion (Flow): 3.9 x 10⁻⁵ /°C
  • Density: 1.32 g/cm³
  • Melt Volume Rate (260°C/5.0 kg): 10 cm³/10 min
  • Injection Molding Guidelines
  • Melt Temperature: 270 – 300 °C
  • Mold Temperature: 60 – 100 °C
  • Drying: 2-6 hours at 110-120 °C

Application

  • Automotive Interior & Exterior Parts:
  • Consumer Electronics Housings
  • Electrical Enclosures

Features & Benefits

Withstands High-Temperature Environments

CYCOLOY CM8823 Resin maintains structural integrity with a Heat Deflection Temperature of 118°C, ensuring parts perform reliably in hot conditions without warping.

Excellent Strength and Stiffness

This material offers high modulus and flexural strength, providing the rigidity needed for large, thin-walled components that must resist bending or breaking under load.

Reliable Impact Resistance

With good notched Izod impact values even at -30°C, CYCOLOY Resin CM8823 helps prevent brittle fractures, ensuring product durability and longevity in tough conditions.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine