CYCOLOY™ Resin CP8320

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy CP8320 (PC/ABS) Resin

Cycoloy Resin CM8320 is a medium-heat PC/ABS blend engineered as a superior plating grade for demanding automotive applications, offering an excellent balance of strength, impact resistance, and thermal performance.

  • Character: Medium Heat Plating Grade for Automotive
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Tensile Strength at Yield: 45 MPa
  • Tensile Modulus: 2100 MPa
  • Flexural Strength at Yield: 70 MPa
  • Izod Impact, Notched (23°C): 600 J/m
  • Heat Deflection Temperature (HDT) @ 1.82 MPa: 92 °C
  • Vicat Softening Temperature (Rate B/50): 106 °C
  • Melt Flow Rate (260°C/5.0 kg): 14 g/10 min
  • Mold Shrinkage, Flow: 0.5 – 0.7 %
  • Specific Gravity: 1.1
  • Melt Temperature: 250 – 280 °C
  • Mold Temperature: 60 – 90 °C
  • Drying Conditions: 2-4 hours at 95-105 °C

Application

  • Automotive Interior Trim Components
  • Automotive Grilles
  • Automotive Emblems and Logos
  • Other Plated Automotive Exterior Parts

Features & Benefits

Superior Impact Resistance & Toughness

With its high Izod and Charpy impact values, this CYCOLOY CM8320 Resin ensures components can withstand physical shocks and stresses, reducing the risk of failure in demanding environments.

Excellent Plating Grade Adhesion

Specifically formulated for plating, it provides a reliable substrate for superior metallic surface finishes, ensuring a high-quality, durable aesthetic for visible automotive parts.

Good Thermal & Dimensional Stability

This resin maintains its properties and shape under high temperatures, making it ideal for parts near engines or in hot climates, and ensuring long-term performance and fit.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top