Sabic Cycoloy CY8630 (PC/ABS) Resin
Cycoloy CY8630 Resin is a high-performance PC/ABS blend engineered for demanding automotive applications, offering an exceptional balance of impact strength, heat resistance, and processability.
- Character: Medium Heat Plating Grade for Automotive
Key technical data
- Tensile Stress at Yield: 58 MPa
- Flexural Modulus: 2300 MPa
- Tensile Strain at Break: 75%
- Izod Impact, Notched (23°C): 600 J/m
- Instrumented Dart Impact Total Energy (23°C): 90 J
- HDT @ 1.82 MPa: 110 °C
- Vicat Softening Temperature (Rate B/50): 131 °C
- Ball Pressure Test (75°C): Passes
- Specific Gravity: 1.15
- Melt Temperature: 260 – 290 °C
- Mold Temperature: 60 – 90 °C