CYCOLOY™ Resin HC1104HF

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy HC1104HF (PC/ABS) Resin

Cycoloy HC1104HF is a high-heat PC/ABS blend engineered for superior impact resistance and excellent flow, making it ideal for demanding, high-performance applications.

  • Character: good flow and excellent impact.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 53 MPa
  • Tensile Modulus: 2250 MPa
  • Flexural Strength at Yield: 83 MPa
  • Izod Impact, Notched (23°C): 583 J/m
  • HDT @ 1.82 MPa: 106 °C
  • HDT @ 0.45 MPa: 128 °C
  • Vicat Softening Temperature: 121 °C
  • Melt Flow Rate (260°C/5.0 kg): 17 g/10 min
  • Recommended Melt Temperature: 260 – 290 °C
  • Recommended Mold Temperature: 60 – 90 °C

Application

  • Automotive Interior Components (e.g., dashboard panels, trim, glove boxes)
  • Consumer Electronics Housings (e.g., laptops, power tool bodies, connectors)
  • Durable Thin-Walled Applications
  • Enclosures Requiring UL Recognition
  • Components Exposed to High Ambient Temperatures

Features & Benefits

Exceptional High-Heat Resistance

With a Heat Deflection Temperature of 106°C at 1.82 MPa, this CYCOLOY HC1104HF Resin withstands high-temperature environments, preventing deformation in applications like automotive interiors and electronics enclosures.

Superior Impact Strength & Durability

It offers excellent notched Izod impact resistance (583 J/m at 23°C), ensuring your products can endure rough handling and sudden impacts without cracking, which enhances product longevity and reduces failure rates.

Excellent Melt Flow for Processing

The high melt flow rate (17 g/10min) allows the HC1104HF to fill complex and thin-walled molds easily, resulting in faster cycle times and improved manufacturing efficiency for intricate part designs.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity