CYCOLOY™ Resin HC1204HF

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy HC1204HF (PC/ABS) Resin

Cycoloy Resins HC1204HF is a high-heat PC/ABS blend engineered for medical and pharmaceutical applications. It combines excellent impact strength, superior flow, and full biocompatibility (ISO 10993/USP Class VI), ensuring reliability for critical healthcare components.

  • Character: good flow and excellent impact
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • HDT @ 1.82 MPa: 112°C (234°F)
  • Vicat Softening Temperature: 130°C (266°F)
  • Tensile Strength at Yield: 57 MPa
  • Flexural Modulus: 2300 MPa
  • Notched Izod Impact @ 23°C: 580 J/m
  • Melt Flow Rate: 24 g/10 min (260°C/5.0kgf)
  • Mold Shrinkage: 0.5 – 0.7%
  • Specific Gravity: 1.15
  • UL 94 HB @ 1.2mm and 3.0mm

Application

  • Medical Device Housings and Enclosures
  • Surgical Instruments and Tooling
  • Pharmaceutical Packaging Components
  • Drug Delivery Systems
  • Durable Laboratory Equipment

Features & Benefits

Withstands Rigorous Sterilization Cycles

This high-heat CYCOLOY HC1204HF Resin maintains structural integrity after repeated autoclaving or steam sterilization, ensuring long-term device reliability and safety for surgical tools and housings.

Exceptional Durability and Impact Resistance

Th

Ou

The h

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity