CYCOLOY™ Resin LG9000

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy LG9000 (PC/ABS) Resin

Cycoloy Resins LG9000 is a premium PC/ABS blend engineered to deliver a consistent low-gloss surface right out of the mold, eliminating the need for secondary finishing and providing excellent impact strength and thermal stability for durable components.

  • Character: low gloss
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 54 MPa
  • Flexural Modulus: 2300 MPa
  • Izod Impact (Notched, 23°C): 534 J/m
  • Heat Deflection Temp (HDT) @ 1.82 MPa: 110 °C
  • Vicat Softening Temperature: 129 °C
  • Specific Gravity: 1.13
  • Mold Shrinkage: 0.5 – 0.7% (SABIC Method)
  • Melt Flow Rate (260°C/5.0kg): 17 g/10 min
  • Gloss (60°): 30 – Confirming low-gloss finish
  • Melt Temperature: 275 – 300 °C
  • Mold Temperature: 60 – 90 °C
  • Drying: 3-4 hours at 105-110 °C

Application

  • Automotive Interiors: Durable, low-gloss components
  • Consumer Electronics: Housings for monitors, printers, and home appliances
  • Industrial Equipment: Housings and covers for machinery

Features & Benefits

Superior Impact Strength at Low Temperatures

With high Izod and dart impact values even at -30°C, LG9000 Resin ensures your products remain tough and crack-resistant in challenging environments, from freezing winters to refrigerated applications.

Excellent Heat Resistance for Assembled Parts

Its high Heat Deflection Temperature (HDT) allows parts to withstand the high heat of assembly processes, such as soldering or hot environments, without warping or losing structural integrity.

Consistent Low-Gloss, Aesthetic Finish

This LG9000 plastic material delivers a uniform low-gloss surface straight from the mold, ideal for consumer electronics and automotive interiors where a premium, non-reflective look is critical, saving on paint and finishing costs.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity