Key technical data

  • Tensile Strength at Yield: 50 MPa
  • Flexural Modulus: 2100 MPa
  • Izod Impact (Notched, 23°C): 534 J/m
  • HDT @ 0.45 MPa: 115 °C
  • HDT @ 1.82 MPa: 99 °C
  • Vicat Softening Temperature: 112 °C
  • Melt Flow Rate (260°C/5.0kg): 14 g/10 min
  • Specific Gravity: 1.1
  • Mold Shrinkage, Flow: 0.5 – 0.8 %

Application

  • Automotive Interior Trims (e.g., plated grilles, painted panels)
  • Consumer Electronics Housings (e.g., laptop bezels, tablet frames)
  • Durable Industrial Components and Housings
  • Household Appliances and Power Tool Casings

Features & Benefits

Superior Impact Strength & Toughness

With high Izod and Charpy impact values, even at low temperatures, CYCOLOY MC1300 ensures your components resist cracking and withstand sudden impacts during assembly and daily use.

Excellent Flow for Complex Molds

Its high melt flow rate allows CYCOLOY Resin MC1300 to easily fill thin walls and intricate mold geometries, reducing injection pressure and minimizing part defects like short shots or weld lines.

High Heat Resistance for Durable Parts

With a Heat Deflection Temperature (HDT) up to 115°C, components made from CYCOLOY MC1300 maintain their structural integrity in high-temperature environments, such as inside automotive interiors or near electronics.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top