Sabic Cycoloy MC8002 (PC/ABS) Resin
Cycoloy Resin MC8002 is a high-performance PC/ABS blend engineered for toughness. It combines low viscosity for easy processing with exceptional impact strength and ductility for durable end-use parts.
- Character: low viscosity, high impact and ductile
Key technical data
- Tensile Strength at Yield: 56 MPa
- Flexural Modulus: 2340 MPa
- Elongation at Break: 150% (High Ductility)
- Notched Izod Impact (23°C): 640 J/m
- Instrumented Dart Impact (23°C): 61 J
- Heat Deflection Temp (1.82 MPa / 6.4mm): 110 °C
- Coefficient of Thermal Expansion: 7.2 x 10⁻⁵ /°C
- Specific Gravity: 1.14
- Melt Flow Rate (260°C/5.0kg): 9 g/10 min
- Mold Shrinkage: 0.5 – 0.7%
- Melt Temperature: 275 – 300 °C
- Mold Temperature: 60 – 90 °C
- Drying: 3-4 hours at 105-110 °C