CYCOLOY™ Resin MC8800

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy MC8800 (PC/ABS) Resin

Cycoloy MC8800 is a high-heat, high-impact PC/ABS plastic resin. It delivers exceptional dimensional stability with a low CTE, making it a robust and reliable choice for demanding applications, particularly in the automotive sector.

  • Character: PC/ABS, high heat, high impact, low CTE.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 55 MPa
  • Flexural Modulus: 2960 MPa
  • Notched Izod Impact (23°C): 427 J/m
  • Heat Deflection Temperature (HDT @ 0.45 MPa): 137°C
  • Vicat Softening Temperature: 117°C
  • Low Coefficient of Thermal Expansion (CTE): 6.66 x 10⁻⁵ /°C
  • Melt Flow Rate (260°C/5.0 kg): 10 g/10 min
  • Specific Gravity: 1.22
  • Mold Shrinkage: 0.4 – 0.6%

Application

  • Automotive Exterior Body Panels
  • Automotive Bumper Fascias
  • Durable Consumer Electronics Housings
  • Industrial Equipment Housings
  • Components Requiring High Heat Resistance

Features & Benefits

Superior Heat & Dimensional Stability

With a Heat Deflection Temperature up to 137°C, CYCOLOY MC8800 maintains its shape and strength under high heat, preventing warping in demanding environments like automotive exteriors.

Exceptional Impact Resistance

This CYCOLOY MC8800 offers outstanding toughness, from room temperature down to -30°C, ensuring your products can withstand sudden impacts and harsh conditions without failing.

Excellent Processing & Flow Characteristics

Its balanced melt flow allows for easier filling of complex molds, enabling faster production cycles and superior surface finish for high-quality, aesthetically pleasing parts.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top