Sabic Cycoloy XCM830 (PC/ABS) Resin
Cycoloy Resin XCM830 is a talc-filled PC/ABS blend engineered for high stiffness and superior impact resistance, making it a robust and reliable choice for demanding structural applications.
- Character: a 8% Talc filled PC/ABS, High stiffness and impact performance.
Key technical data
- Tensile Stress at Yield: 60 MPa
- Flexural Modulus: 3100 MPa
- Izod Impact, Notched (23°C): 500 J/m
- Heat Deflection Temperature (HDT @ 1.82 MPa): 118 °C
- Vicat Softening Temperature (Rate B/50): 138 °C
- Ball Pressure Test (125°C): Passes (IEC 60695-10-2)
- Specific Gravity: 1.22
- Melt Flow Rate (260°C/5.0 kg): 11 g/10 min
- Mold Shrinkage, Flow: 0.7 – 0.8 %
Application
- Automotive Interior Components (e.g., brackets, supports, and trim)
- Durable Consumer and Electronics Housings
- Industrial Equipment Housings and Covers
- Structural Parts Requiring High Rigidity and Toughness
Features & Benefits

Related CYCOLOY™ PC/ABS Products
CYCOLOY™ Resin XCM830
CYCOLOY™ Resin MC8800
CYCOLOY™ Resin MC8100
CYCOLOY™ Resin MC8002
CYCOLOY™ Resin MC1300
CYCOLOY™ Resin LG9000
CYCOLOY™ Resin HC1204HF
CYCOLOY™ Resin HC1104HF
CYCOLOY™ Resin CY8630
CYCOLOY™ Resin CP8320
CYCOLOY™ Resin CM8823
CYCOLOY™ Resin CM8622
CYCOLOY™ Resin C4220
CYCOLOY™ Resin C4210HF
CYCOLOY™ Resin C1200HF
Advanced Manufacturing