CYCOLOY™ Resin XCY620S

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy XCY620S (PC/ABS) Resin

Cycoloy Resin XCY620S is a hydrolytically stable PC/ABS blend, available in standard black and natural colors. It delivers an exceptional balance of strength, impact resistance, and thermal stability for demanding engineering applications.

  • Character: PC/ABS, hydrolytically stable, standard black and natural.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Stress at Yield: 54 MPa (ISO 527)
  • Flexural Modulus: 2300 MPa (ASTM D790)
  • Izod Impact, Notched (23°C): 55 kJ/m² (ISO 180)
  • Instrumented Dart Impact (23°C): 55 J (ASTM D3763)
  • Heat Deflection Temp (HDT) @ 1.82 MPa: 108°C (ASTM D648)
  • Vicat Softening Temperature: 129°C (ASTM D1525)
  • Ball Pressure Test (75°C): Passes (IEC 60695-10-2)
  • Specific Gravity: 1.14
  • Melt Temperature: 260 – 290 °C
  • Mold Temperature: 60 – 90 °C
  • Mold Shrinkage: 0.5 – 0.7%

Application

  • Automotive Interior Components (e.g., dashboard panels, trim)
  • Consumer Electronics Housings (e.g., power tools, appliance covers)
  • Enclosures for Electrical Equipment
  • Components Requiring UL Recognition

Features & Benefits

Superior Impact Strength & Toughness

With high notched Izod and instrumented dart impact values, CYCOLOY XCY620S withstands sudden impacts and rough handling, reducing part failure and returns in durable goods.

Excellent Hydrolytic Stability

This XCY620S plastic formulation resits moisture absorption, ensuring long-term property retention and dimensional stability in humid environments, which is critical for exterior components.

High Heat Resistance & Stability

It maintains structural integrity with a Heat Deflection Temperature of 108°C (1.82 MPa), making CYCOLOY XCY620S ideal for applications exposed to elevated temperatures during use or assembly.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing