SABIC® PC Resin ALS01

SABIC® PC Resin

Sabic PC Resin ALS01 Injection Molding Grade

Sabic PC ALS01 is a medium-flow, heat and UV-stabilized polycarbonate with mold release, engineered specifically for high-performance automotive lens applications. It delivers exceptional clarity, durability, and processability.

  • Character: medium-low flow (MFR13), heat and UV stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Melt Flow Rate (300°C/1.2 kg): 13 g/10 min
  • Light Transmission (2.54 mm): 88 – 90 %
  • Haze (2.54 mm): < 0.8 %
  • Heat Deflection Temp (HDT @ 1.82 MPa): 127 °C
  • Izod Impact, Notched (23°C): 800 J/m (ASTM)
  • Vicat Softening Temperature: 143 °C
  • Tensile Strength at Yield: 63 MPa
  • Mold Shrinkage, Flow: 0.5 – 0.7 %
  • Rockwell Hardness (R Scale): 120

Application

  • Headlamp Lenses
  • Fog Lamp Lenses
  • Daytime Running Light (DRL) Lenses
  • Signal Light Lenses (Turn Indicators, Stop Lights)

Features & Benefits

Superior Impact Resistance

With its no-break unnotched Izod impact, SABIC PC Resin ALS01 ensures lenses resist shattering from road debris, enhancing safety and reducing warranty claims.

Excellent Optical Clarity

It offers high light transmission (88-90%) and low haze, creating brighter, more efficient lighting for automotive signals and headlamps, improving vehicle visibility and safety.

Reliable High-Temperature Performance

A high Heat Deflection Temperature (HDT) ensures lenses maintain their shape and integrity under the high heat generated by modern LED and halogen lighting systems.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine