Sabic PC0703R is a low-flow, extrusion-grade polycarbonate. It is heat and UV stabilized with an internal mold release, engineered for superior performance in demanding profile and sheet applications.

  • Character: low flow (MFR = 7 at 300°C/1.2kg), heat and UV stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Stress at Yield: 63 MPa
  • Flexural Modulus: 2300 MPa
  • Notched Izod Impact (23°C): 900 J/m (ASTM) / 70 kJ/m² (ISO)
  • Heat Deflection Temp (HDT) @ 1.82 MPa: 127°C
  • Vicat Softening Temperature: 144°C
  • Ball Pressure Test (125°C): Passes
  • Melt Flow Rate (300°C/1.2kg): 7 g/10 min
  • Mold Shrinkage: 0.5 – 0.7%
  • Recommended Melt Temp (Extrusion): 270 – 280 °C

Application

  • Protective and Security Glazing
  • Industrial Machine Guards and Housings
  • Continuous Profiled Sheets and Multiwall Panels
  • Automotive Components
  • Electrical Enclosures requiring UL recognition

Features & Benefits

Exceptional Impact Strength

With its high notched Izod impact, Sabic PC0703R produces tough, durable parts that resist cracking and withstand physical abuse, reducing failure rates in the field.

Reliable Heat Resistance

This material maintains structural integrity under high temperatures, passing critical thermal tests like the Ball Pressure Test for electrical safety applications.

Optimized for Extrusion

The low melt flow of SABIC PC Resin PC0703R ensures excellent melt strength for stable, consistent profiles and sheets, streamlining your production process.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top